公开(公告)号:US20090054568A1
公开(公告)日:2009-02-26
申请号:US11912896
申请日:2006-04-14
CPC分类号: C08L69/00 , C08K5/521 , C08L25/12 , C08L51/04 , C08L67/02 , C08L2666/14 , C08L2666/02 , C08L2666/24
摘要: The objective of the present invention is to provide a thermoplastic resin composition excelling in translucency, impact resistance, heat resistance and fluidity, particularly a thermoplastic resin composition that in the production of thermoplastic resin molded items through extrusion processing, molding processing, etc., permits a wide tolerance range of processing conditions, such as low susceptibility to quality deterioration by thermal history, excelling in translucency, impact resistance, heat resistance and fluidity; and a molding thereof. The present composition comprises a rubber-reinforced resin consisting of a rubber-reinforced copolymeric resin obtained by polymerization of a vinyl-based monomer including an aromatic vinyl compound in the presence of a rubbery polymer having refractive index in the range from 1.520-1.580, or a mixture of this rubber-reinforced copolymeric resin and a (co)polymer of the above vinyl-based monomer, and a polycarbonate resin in specified ratio, and further comprises a phosphoric compound.
摘要翻译: 本发明的目的是提供一种在半透明性,耐冲击性,耐热性和流动性方面优异的热塑性树脂组合物,特别是热塑性树脂组合物,其通过挤出加工,模塑加工等生产热塑性树脂模塑制品,允许 处理条件的宽公差范围,如热历史对质量劣化的敏感性低,半透明性,耐冲击性,耐热性和流动性优异; 及其成型品。 本发明的组合物包含橡胶强化树脂,该树脂由在具有1.520-1.580范围内的折射率的橡胶状聚合物存在下聚合包含芳香族乙烯基化合物的乙烯基类单体得到的橡胶增强共聚树脂,或 该橡胶增强共聚树脂与上述乙烯基类单体的(共)聚合物和特定比例的聚碳酸酯树脂的混合物,还包含磷化合物。