公开(公告)号:US09160002B2
公开(公告)日:2015-10-13
申请号:US13818761
申请日:2011-01-17
CPC分类号: H01M4/583 , H01M4/14 , H01M4/62 , H01M4/625 , H01M4/628 , H01M10/121 , H01M10/4235 , H01M10/44 , H01M2004/021 , H01M2004/027 , Y02E60/126 , Y02T10/7016
摘要: In a valve-regulated lead-acid battery in which charging is performed intermittently on every short time and high rate discharging to a load is performed in a partial state of charge (PSOC), a valve-regulated lead-acid battery improved for the charge acceptance and the life characteristic under PSOC than usual is provided. A positive electrode plate having a specific surface area of an active material of 5.5 m2/g or more is used. A valve-regulated lead-acid battery is manufactured by using a negative electrode plate improved for the charge acceptance and the life performance by adding a carbonaceous electroconductive material and a formaldehyde condensate of bisphenols aminobenzene sulfonic acid to a negative electrode active material and setting the specific gravity of an electrolyte to 1.30 or more and 1.35 or less.
摘要翻译: 在部分充电状态(PSOC)中,在每隔短时间间歇地进行充电进行负荷的高速率放电的阀控式铅酸电池中,对于充电状态进行了改善的阀控式铅酸蓄电池 提供PSOC以下的接受和生活特征。 使用活性物质的比表面积为5.5m 2 / g以上的正极板。 通过使用通过将碳导电材料和双酚氨基苯磺酸的甲醛缩合物加入到负极活性材料中,通过使用改进的充电接受性和寿命性能的负极板来制造阀控铅酸蓄电池, 电解液的重力为1.30以上且1.35以下。
-
公开(公告)号:US20130157118A1
公开(公告)日:2013-06-20
申请号:US13818761
申请日:2011-01-17
IPC分类号: H01M4/583
CPC分类号: H01M4/583 , H01M4/14 , H01M4/62 , H01M4/625 , H01M4/628 , H01M10/121 , H01M10/4235 , H01M10/44 , H01M2004/021 , H01M2004/027 , Y02E60/126 , Y02T10/7016
摘要: In a valve-regulated lead-acid battery in which charging is performed intermittently on every short time and high rate discharging to a load is performed in a partial state of charge (PSOC), a valve-regulated lead-acid battery improved for the charge acceptance and the life characteristic under PSOC than usual is provided. A positive electrode plate having a specific surface area of an active material of 5.5 m2/g or more is used. A valve-regulated lead-acid battery is manufactured by using a negative electrode plate improved for the charge acceptance and the life performance by adding a carbonaceous electroconductive material and a formaldehyde condensate of bisphenols aminobenzene sulfonic acid to a negative electrode active material and setting the specific gravity of an electrolyte to 1.30 or more and 1.35 or less.
摘要翻译: 在部分充电状态(PSOC)中,在每隔短时间间歇地进行充电进行负荷的高速率放电的阀控式铅酸电池中,对于充电状态进行了改善的阀控式铅酸蓄电池 提供PSOC以下的接受和生活特征。 使用活性物质的比表面积为5.5m 2 / g以上的正极板。 通过使用通过将碳导电材料和双酚氨基苯磺酸的甲醛缩合物加入到负极活性材料中,通过使用改进的充电接受性和寿命性能的负极板来制造阀控铅酸蓄电池, 电解液的重力为1.30以上且1.35以下。
-
公开(公告)号:US20130022860A1
公开(公告)日:2013-01-24
申请号:US13581657
申请日:2010-12-27
申请人: Satoshi Minoura , Toshio Shibahara , Masanori Sakai , Koji Kogure
发明人: Satoshi Minoura , Toshio Shibahara , Masanori Sakai , Koji Kogure
CPC分类号: H01M4/14 , H01M2/1666 , H01M4/625 , H01M4/628 , H01M10/06 , H01M2004/021 , Y02E60/126 , Y02T10/7016
摘要: A flooded-type lead acid storage battery in which charging is intermittently carried out in a short period of time and high-efficiency discharge to a load is carried out in a partial state of charge, wherein the charge acceptance and service life characteristics are improved by using a positive plate in which the specific surface area of the active material is set to 6 m2/g or more; a negative plate with improved charge acceptance and service life performance obtained by adding a carbonaceous electrically conductive material, and a bisphenol aminobenzenesulfonic acid formaldehyde condensate to the negative active material; and a separator formed from a nonwoven in which the surface facing the negative plate is composed of material selected from glass, pulp, and polyolefin.
摘要翻译: 在部分充电状态下进行在短时间内间歇地进行充电并对负载进行高效率放电的淹水式铅酸蓄电池,其中充电接收和使用寿命特性通过 使用将活性物质的比表面积设定为6m 2 / g以上的正极板; 通过向负极活性物质中添加碳质导电材料和双酚氨基苯磺酸甲醛缩合物而获得的具有改善的电荷接受性和使用寿命性能的负极板; 以及由非织造材料形成的隔板,其中面向负极板的表面由选自玻璃,纸浆和聚烯烃的材料构成。
-
公开(公告)号:US09735409B2
公开(公告)日:2017-08-15
申请号:US14117106
申请日:2012-02-28
申请人: Masatoshi Toduka , Masanori Sakai , Shinsuke Kobayashi , Koji Kogure , Satoshi Minoura , Toshio Shibahara
发明人: Masatoshi Toduka , Masanori Sakai , Shinsuke Kobayashi , Koji Kogure , Satoshi Minoura , Toshio Shibahara
CPC分类号: H01M2/162 , H01M2/1606 , H01M4/14 , H01M4/621 , H01M4/685 , H01M10/06 , H01M10/128 , H01M10/4235 , H01M2220/20 , H01M2300/0011 , Y02E60/126
摘要: On each negative plate (1), a non-woven fabric (2) composed of fibers of at least one material selected from a group of materials comprising glass, pulp and polyolefins comes into contact with the entire surface of the plate without being integrated with the plate. Each negative plate (1), which is in contact with the non-woven fabric (2), is contained in an envelope separator (3) comprising a microporous synthetic resin sheet, and is laminated with a positive plate (4). The non-woven fabric is manufactured through papermaking process in which glass fibers, pulp and silica powder are preferably used and dispersed in water as the main components.
-
公开(公告)号:US20130099749A1
公开(公告)日:2013-04-25
申请号:US13696599
申请日:2011-03-16
IPC分类号: H02J7/00
CPC分类号: H02J7/00 , H01M4/14 , H01M4/62 , H01M4/625 , H01M10/12 , H01M10/44 , H01M2004/021 , Y02E60/126 , Y02T10/7016
摘要: A flooded-type lead-acid battery in which charging is intermittently carried out in a short period of time and high-rate discharge to a load is carried out in a partial state of charge, wherein the charge acceptance and service life characteristics under PSOC are improved by using a positive plate in which the total surface area of the positive active material per unit of the plate pack volume is set in a range of 3.5 to 15.6 m2/cm3; a negative plate with improved charge acceptance and service life performance obtained by adding a carbonaceous electrically conductive material, and a formaldehyde condensate of bisphenol and aminobenzene sulfonic acid to the negative active material; and a separator formed from a nonwoven in which a surface facing the negative plate is composed of material selected from glass, pulp, and polyolefin.
摘要翻译: 在部分充电状态下进行短时间间歇地进行充电并向负载高速率放电的淹水式铅酸蓄电池,其中PSOC下的充电接受和使用寿命特性为 通过使用正极板改善,其中每单位板组件容积的正极活性材料的总表面积设定在3.5至15.6m 2 / cm 3的范围内; 通过将碳质导电材料和双酚和氨基苯磺酸的甲醛缩合物加入到负极活性物质中而获得的具有改善的充电接受性和使用寿命性能的负极板; 以及由非织造材料形成的隔板,其中面向负极板的表面由选自玻璃,纸浆和聚烯烃的材料构成。
-
公开(公告)号:US20150050540A1
公开(公告)日:2015-02-19
申请号:US14117106
申请日:2012-02-28
CPC分类号: H01M2/162 , H01M2/1606 , H01M4/14 , H01M4/621 , H01M4/685 , H01M10/06 , H01M10/128 , H01M10/4235 , H01M2220/20 , H01M2300/0011 , Y02E60/126
摘要: On each negative plate (1), a non-woven fabric (2) composed of fibers of at least one material selected from a group of materials comprising glass, pulp and polyolefins comes into contact with the entire surface of the plate without being integrated with the plate. Each negative plate (1), which is in contact with the non-woven fabric (2), is contained in an envelope separator (3) comprising a microporous synthetic resin sheet, and is laminated with a positive plate (4). The non-woven fabric is manufactured through papermaking process in which glass fibers, pulp and silica powder are preferably used and dispersed in water as the main components.
摘要翻译: 在每个负极板(1)上,由选自玻璃,纸浆和聚烯烃的材料组中的至少一种材料的纤维构成的无纺布(2)与板的整个表面接触而不与 碟子。 与无纺布(2)接触的负极板(1)包含在包含微孔合成树脂片材的包层隔板(3)中,并与正极板(4)层叠。 通过造纸方法制造无纺布,其中优选使用玻璃纤维,纸浆和二氧化硅粉末并分散在水中作为主要成分。
-
公开(公告)号:US20130029210A1
公开(公告)日:2013-01-31
申请号:US13581664
申请日:2011-01-07
IPC分类号: H01M2/02
CPC分类号: H01M2/1633 , H01M4/14 , H01M4/621 , H01M4/622 , H01M4/625 , H01M4/627 , H01M10/06 , Y02E60/126 , Y02T10/7016
摘要: In a liquid-type lead acid storage battery in which charging is performed for a short time intermittently and high-rate discharging to load is performed in a partially charged state, there are used a positive electrode plate in which the utilization rate of a positive electrode activation substance is set to a range of 50% to 65%, and a negative electrode plate in which a carbonaceous electroconductive material and a bisphenol/aminobenzenesulfonic acid/formaldehyde condensate are added to the negative electrode activation substance, thereby improving the charge acceptance and the lifespan performance; and a separator whose surface disposed opposite the negative electrode plate is formed from a nonwoven fabric made of a material selected from glass, pulp, and polyolefin, is used as a separator; whereby the charge acceptance and the lifespan performance under PSOC are improved.
摘要翻译: 在部分充电状态下,在短时间内进行充电且负荷高速放电的液体型铅酸蓄电池中,使用正极板,其中正极 将活化物质设定为50〜65%的范围,在负极活性物质中添加碳质导电性物质和双酚/氨基苯磺酸/甲醛缩合物的负极板,从而提高电荷接受性, 寿命表现; 并且使用由选自玻璃,纸浆和聚烯烃的材料制成的无纺布形成的与负极板相对的表面的隔板用作隔膜; 从而提高了PSOC下的充电接受度和使用寿命。
-
公开(公告)号:US06366055B1
公开(公告)日:2002-04-02
申请号:US09816145
申请日:2001-03-26
申请人: Tetsuro Ookoshi , Satoshi Minoura , Tokiyoshi Hirasawa , Yoshinari Morimoto , Ichiro Shimoura , Yoshihisa Okuda , Kenichi Maeda , Keizo Yamada
发明人: Tetsuro Ookoshi , Satoshi Minoura , Tokiyoshi Hirasawa , Yoshinari Morimoto , Ichiro Shimoura , Yoshihisa Okuda , Kenichi Maeda , Keizo Yamada
IPC分类号: H02J714
CPC分类号: H02J7/1423 , B60R16/03
摘要: A power system where energy generated at a deceleration time of a running vehicle such as an automobile can be accepted as regenerative energy sufficiently and safely is provided. In a power system 10, a non-aqueous solution system secondary battery group 1 where 10 to 11 lithium ion secondary battery cells are connected in series and an aqueous solution system secondary battery group 2 where 18 control valve type lead-acid battery cells are connected in series are connected in parallel. The battery capacity of the non-aqueous solution system secondary battery group 1 is smaller than that of the aqueous solution system secondary battery group 2. The non-aqueous solution system secondary battery group 1 and the aqueous solution system secondary battery group 2 are charged at a current value of 7C or less from a motor generator 3, and the ratio of the charged current value of the aqueous solution system secondary battery group 2 to the charged current value of the non-aqueous solution system secondary battery group 1 is 0.05 to 1.00.
摘要翻译: 能够充分,安全地接受作为汽车等行驶车辆的减速时间产生的能量作为再生能量的电力系统。 在电力系统10中,连接有10〜11个锂离子二次电池单体的非水溶液系统二次电池组1和18个控制阀型铅酸电池单元连接的水溶液系统二次电池组2 串联并联。 非水溶液系统二次电池组1的电池容量小于水溶液系统二次电池组2的电池容量。非水溶液系统二次电池组1和水溶液系统二次电池组2充电在 电动发电机3的电流值为7C以下,水溶液系二次电池组2的充电电流值与非水溶液系二次电池组1的充电电流值的比为0.05〜1.00 。
-
-
-
-
-
-
-