Heat sealable laminated propylene polymer packaging material
    1.
    发明授权
    Heat sealable laminated propylene polymer packaging material 失效
    可热封层压丙烯聚合物包装材料

    公开(公告)号:US4230767A

    公开(公告)日:1980-10-28

    申请号:US10641

    申请日:1979-02-08

    摘要: A packaging material having an excellent seal packaging property, which comprises (A) a base layer consisting of a stretched film made of a polymer composition comprising a propylene polymer and (B) a surface layer consisting of a stretched film made of a polymeric mixture comprising a polymer blend provided on at least one surface of said base layer, said polymer blend comprising a copolymer of ethylene and propylene and a copolymer of butene and any other polymerizable monomer having an ethylenic unsaturation in a weight proportion of 5:95 to 95:5.

    摘要翻译: 一种具有优异的密封封装性的包装材料,其包括(A)由包含丙烯聚合物的聚合物组合物制成的拉伸膜组成的基层和(B)由聚合物混合物制成的拉伸膜组成的表面层,所述拉伸膜包含 提供在所述基层的至少一个表面上的聚合物共混物,所述聚合物共混物包含乙烯和丙烯的共聚物和丁烯与任何其它可聚合单体的共聚物,其重量比例为5:95至95:5 。

    Composite film and packaging material of polypropylene base and surface
polymer composition
    2.
    发明授权
    Composite film and packaging material of polypropylene base and surface polymer composition 失效
    聚丙烯基复合膜和包装材料和表面聚合物组成

    公开(公告)号:US4343852A

    公开(公告)日:1982-08-10

    申请号:US167736

    申请日:1980-07-14

    摘要: A packaging material which is capable of packaging an article(s) in a closely fitted and tightly sealed state and consists essentially of a composite film stretched at least in one direction,said composite film comprising a base film and a surface film provided on at least one surface of the base film and having certain specific shrinkage characteristics,said base film being made of a resin composition comprising a propylene polymer, andsaid surface film being made of a polymer composition comprising at least two of (A) a copolymer of propylene and ethylene in a weight proportion of 99.5:0.5 to 90:10, (B) a copolymer of propylene and an .alpha.-olefin having 4 to 10 carbon atoms in a weight proportion of 70:30 to 95:5 and (C) a copolymer of butene and any other .alpha.-olefin having 2 to 10 carbon atoms in a weight proportion of 70:30 to 99:1, each of the copolymers being in an amount of 10 to 90% by weight on the total weight of the copolymers.

    摘要翻译: 一种包装材料,其能够以紧密配合和紧密密封的状态包装物品,并且基本上由至少沿一个方向拉伸的复合膜组成,所述复合膜包括基膜和至少提供的表面膜 所述基膜由包含丙烯聚合物的树脂组合物制成,所述表面膜由聚合物组合物制成,所述聚合物组合物包含(A)丙烯和 乙烯的重量比为99.5:0.5至90:10,(B)丙烯与碳原子数为4〜10的α-烯烃的重量比为70:30〜95:5的共聚物,(C)共聚物 的丁烯和任何其它具有2-10个碳原子的α-烯烃,其重量比为70:30至99:1,每个共聚物的量为共聚物总重量的10至90重量%。

    Polyester film
    3.
    发明授权
    Polyester film 失效
    聚酯薄膜

    公开(公告)号:US4264667A

    公开(公告)日:1981-04-28

    申请号:US908656

    申请日:1978-05-23

    摘要: A transparent polyester film having excellent antistatic properties, which are little effected with variation of the humidity, and further having excellent flexing resistance, pinhole resistance and printability, which is made from a mixture comprising (i) a polyester consisting essentially of a residue of dibasic acids wherein at least 80% by mol is terephthalic acid and a residue of at least one glycol and (ii) a block copolyester consisting of a crystalline polyester segment having a high melting point and a soft polymer segment having a low melting point and a number average molecular weight of 400 to 8,000, said soft polymer segment having a low melting point being contained in an amount of 0.5 to 10% by weight on the basis of the whole weight of the components (i) and (ii), and (iii) a sulfonic and/or phosphoric acid metal salt having a good heat resistance, and which is produced by melt-extruding the mixture of the components (i), (ii) and (iii), drawing at least uniaxially and then heat-treating the resultant at a temperature of 170.degree. C. or higher and lower than the melting point of the polyester (i).

    摘要翻译: 具有优异的抗静电性的透明聚酯膜,其几乎不受湿度的变化影响,并且还具有优异的抗弯曲性,针孔抗性和可印刷性,其由以下组成的混合物制成:(i)基本上由二元碱 酸,其中至少80摩尔%为对苯二甲酸和至少一种二醇的残基,和(ii)由具有高熔点的结晶聚酯链段和具有低熔点和数目的软聚合物链段组成的嵌段共聚酯 基于组分(i)和(ii)的总重量,所述软聚合物链段的低熔点含量为0.5〜10重量%,(iii) )具有良好耐热性的磺酸和/或磷酸金属盐,并且通过熔融挤出组分(i),(ii)和(iii)的混合物制备,至少拉伸单轴和 然后在170℃以上且低于聚酯(i)的熔点的温度下对所得物进行热处理。