Abstract: A core material contains Mn: 0.3-2.0 mass % (hereinafter, abbreviated to %), Si: 1.5% or less, Fe: 0.1-1.0% and Cu: 0.05-1.0%, and comprises a remainder Al and unavoidable impurities, and the sacrificial anode material contains Fe: 0.05-1.0% and Zn: 0.5-5.0%, and comprises a remainder Al and unavoidable impurities. A potential at the joint section between the header pipe and the tube is lower by 30 mV or less than potentials at the header pipe surface and the tube surface, and the potential at the joint section is lower by 30-100 mV than a potential at a position in a depth of one quarter of the overall thickness from the header pipe surface and a potential at a position in a depth of one quarter of the overall thickness from the tube surface.
Abstract translation: 芯材含有Mn:0.3〜2.0质量%(以下简称为%),Si:1.5%以下,Fe:0.1〜1.0%,Cu:0.05〜1.0%,其余为Al和不可避免的杂质, 牺牲阳极材料含有Fe:0.05-1.0%和Zn:0.5-5.0%,并且包含剩余的Al和不可避免的杂质。 集管和管之间的连接部分的电位比总管表面和管表面的电位低30 mV或更小,并且接头部分的电位低于30-100 mV时的电位 从总管表面的总厚度的四分之一深度的位置和在距离管表面的总厚度的四分之一深度的位置处的电位。