摘要:
Disclosed are amorphous polyesters that contain only renewable resources designed for emulsion aggregation toner fabrication. The amorphous polyesters may be obtained from the mixture of three different monomers: 1,4:3,6-dianhydro-D-sorbitol (isosorbide), nonanedioic acid (azelaic acid), and butanedioic acid (succinic acid). Different polymer properties may be achieved depending on the ratio of these three monomers. By altering the ratio, polymers of high to low acid value can be obtained, as well as different ranges of glass transition temperatures.
摘要:
Disclosed are amorphous polyesters that contain only renewable resources designed for emulsion aggregation toner fabrication. The amorphous polyesters may be obtained from the mixture of three different monomers: 1,4:3,6-dianhydro-D-sorbitol (isosorbide), nonanedioic acid (azelaic acid), and butanedioic acid (succinic acid). Different polymer properties may be achieved depending on the ratio of these three monomers. By altering the ratio, polymers of high to low acid value can be obtained, as well as different ranges of glass transition temperatures.
摘要:
Environmentally friendly toner particles are provided which may include a bio-based amorphous polyester resin, optionally in combination with another amorphous resin and/or a crystalline resin. Methods for providing these toners are also provided.
摘要:
A toner having an amorphous resin, a crystalline resin, and a colorant, wherein the crystalline resin has a melting temperature of at least 70° C. and a recrystallization point of at least 47° C. exhibits improved document offset properties and improved heat cohesion. Annealing the toner further improves the heat cohesion and morphology of the toner.
摘要:
A toner having an amorphous resin, a crystalline resin, and a colorant, wherein the crystalline resin has a melting temperature of at least 70° C. and a recrystallization point of at least 47° C. exhibits improved document offset properties and improved heat cohesion. Annealing the toner further improves the heat cohesion and morphology of the toner.
摘要:
Environmentally friendly toner particles are provided which may include a bio-based amorphous polyester resin, optionally in combination with another amorphous resin and/or a crystalline resin. Methods for providing these toners are also provided.
摘要:
A toner having an amorphous resin, a crystalline resin, and a colorant, wherein the crystalline resin has a melting temperature of at least 70° C. and a recrystallization point of at least 47° C. exhibits improved document offset properties and improved heat cohesion. Annealing the toner further improves the heat cohesion and morphology of the toner.
摘要:
Polymer particles comprising a cross-linked polymer core and a linear non-cross-linked polymer shell may be formed by emulsion polymerization. The polymer particles may be used in forming toner.
摘要:
Environmentally friendly toner particles are provided which may, in embodiments, include a bio-based amorphous polyester resin, optionally in combination with another amorphous resin and/or a crystalline resin. Toner particles may, in embodiments, have a core-shell configuration, with the shell formed of the bio-based amorphous polyester resin, the amorphous polyester resin, the crystalline polyester resin, or combinations thereof.
摘要:
Environmentally friendly toner particles are provided which may, in embodiments, include a bio-based amorphous polyester resin, optionally in combination with another amorphous resin and/or a crystalline resin. Toner particles may, in embodiments, have a core-shell configuration, with the shell formed of the bio-based amorphous polyester resin, the amorphous polyester resin, the crystalline polyester resin, or combinations thereof.