Process for making-up polyamide resins solid at room temperature
    1.
    发明授权
    Process for making-up polyamide resins solid at room temperature 失效
    室温聚酰胺树脂固化方法

    公开(公告)号:US06232436B1

    公开(公告)日:2001-05-15

    申请号:US09396906

    申请日:1999-09-15

    IPC分类号: C08F600

    CPC分类号: B29B9/065 B29K2077/00

    摘要: A process for granulating a polyamide resin involving: (a) providing an underwater granulating device having a heated multiple-bore die wherein the bores have an internal diameter ranging from 1.2 to 2.5 mm and a length of from 12 to 50 mm; (b) providing a polyamide resin melt having a viscosity, at 160° C., of less than 3,000 mPas; (c) cooling the polyamide resin melt to form a cooled polyamide resin; (d) introducing the cooled polyamide resin into and through the heated multiple-bore die to form an extrudate; (e) providing a source of water; (f) contacting the extrudate with the water to form a cooled extrudate; and (g) cutting the cooled extrudate into granules.

    摘要翻译: 一种用于造粒聚酰胺树脂的方法,包括:(a)提供具有加热的多孔模具的水下造粒装置,其中所述孔的内径为1.2至2.5mm,长度为12至50mm; (b)提供在160℃下粘度小于3,000mPas的聚酰胺树脂熔体; (c)冷却聚酰胺树脂熔体以形成冷却的聚酰胺树脂; (d)将经冷却的聚酰胺树脂引入并通过加热的多孔模具以形成挤出物; (e)提供水源; (f)使挤出物与水接触以形成冷却的挤出物; 和(g)将冷却的挤出物切割成颗粒。