公开(公告)号:US20150322546A1
公开(公告)日:2015-11-12
申请号:US14650245
申请日:2014-05-21
发明人: Songlin Zhou , Weidong Liu , Hu Wang
CPC分类号: A61K39/39558 , A61K38/00 , A61K45/06 , A61K47/6849 , A61K49/04 , A61K49/16 , A61K51/1027 , A61K51/1093 , A61K2039/505 , C07K16/18 , C07K16/28 , C07K16/2836 , C07K2319/74 , C22B7/04 , C22B15/0028 , C22B15/0054 , F27B3/02 , F27B3/205 , F27B9/047 , F27B9/39 , F27D2007/063 , Y02P10/212
摘要: A method and device for producing a crude copper. The method comprises: mixing and reacting copper smelting molten slag (1), a carbon-containing reductant (2) and an inert gas (3) under pressure, the pressure of the inert gas (3) being 100 kPa to 800 kPa. The device comprises: a furnace body (4) and gas nozzles (411) disposed on the furnace body (4), the gas nozzles (411) being located on the sidewall of the furnace body (4) and connected to the center of the molten pool.
摘要翻译: 一种生产粗铜的方法和装置。 该方法包括:将铜熔炼熔渣(1),含碳还原剂(2)和惰性气体(3)在压力下混合和反应,惰性气体(3)的压力为100kPa至800kPa。 该装置包括:炉体(4)和设置在炉体(4)上的气体喷嘴(411),气体喷嘴(411)位于炉体(4)的侧壁上并连接到炉体 熔池。
-
公开(公告)号:US20150307959A1
公开(公告)日:2015-10-29
申请号:US14649800
申请日:2014-05-21
发明人: Songlin Zhou , Weidong Liu , Hu Wang
CPC分类号: C22B7/04 , C22B15/0002 , C22B15/0028 , C22B15/0047 , C22B15/0054 , F27B3/02 , F27B3/205 , F27B14/00 , F27B2014/002 , F27B2014/004 , F27D3/00 , F27D3/0033 , F27D7/02 , F27D99/0033 , Y02P10/212
摘要: A method and device for depleting copper smelting slag. The method comprises mixing copper smelting molten slag (1) with a reductant (2) and an inert gas (3) under pressure, and then depleting same. The device for depletion comprises a furnace body (4), which furnace body (4) is provided with a feed opening (413) and a slag discharge port (416), and gas nozzles (411) disposed on the side wall of the furnace body.
摘要翻译: 一种消耗铜冶炼炉渣的方法和装置。 该方法包括将铜熔炼熔渣(1)与还原剂(2)和惰性气体(3)在压力下混合,然后耗尽。 用于耗尽的装置包括炉体(4),该炉体(4)设置有进料口(413)和排渣口(416),以及设置在炉的侧壁上的气体喷嘴(411) 身体。
-