Process for Preparing Various Morphology NTE Compound ZrW0.5Mo1.5O8
    1.
    发明申请
    Process for Preparing Various Morphology NTE Compound ZrW0.5Mo1.5O8 有权
    制备各种形态NTE化合物ZrW0.5Mo1.5O8的方法

    公开(公告)号:US20120137960A1

    公开(公告)日:2012-06-07

    申请号:US13320137

    申请日:2009-08-27

    IPC分类号: C30B7/10 B82Y30/00 B82Y40/00

    摘要: A process for preparing various morphology NTE compound ZrW0.5Mo1.5O8 comprising: preparing 0.4M Zr4+ solution, 0.2M W6+ solution and 0.6M Mo6+ solution with zirconyl nitrate, ammonium tungstate and ammo-nium molybdate separately, mixing them with the same volume and stirring until they are mixed well, adding 6-12M hydrochloric acid with the volume of ⅕- 1/7 of the mixed solution, or adding 6-12M hydrochloric acid with the volume of ⅓-⅕ of the mixed solution and 0.2-0.4 wt % ammonium monoacid phosphate of all raw materials, or adding 9-18M sulfuric acid with the volume of 1/10-⅕ of the mixed solution, well mixing, transferring the mixed solution into the hydrothermal reactor, reacting at 150-180° C. for 8-25 hours, washing, drying and getting the precursor, heating the precursor at 480-500° C. for more than 5 hours and obtaining the product is provided.

    摘要翻译: 制备各种形态NTE化合物ZrW0.5Mo1.5O8的方法,包括:分别制备0.4M Zr4 +溶液,0.2M W6 +溶液和0.6M Mo6 +溶液,分别用硝酸锆铵,钨酸铵和钼酸铵,将它们与相同体积和 搅拌至充分混合,加入6〜12M盐酸,混合溶液的体积为⅕〜1/7,或加入6-12M盐酸,体积为混合溶液的1/3〜 所有原料的一铵磷酸铵,或加入体积为混合溶液1/10-adding的9-18M硫酸,充分混合,将混合溶液转移到水热反应器中,在150-180℃下反应 8-25小时,洗涤,干燥并得到前体,在480-500℃下加热前体超过5小时,得到产物。

    Process for preparing various morphology NTE compound ZrW0.5Mo1.5O8
    2.
    发明授权
    Process for preparing various morphology NTE compound ZrW0.5Mo1.5O8 有权
    制备各种形态NTE化合物ZrW0.5Mo1.5O8的方法

    公开(公告)号:US09090480B2

    公开(公告)日:2015-07-28

    申请号:US13320137

    申请日:2009-08-27

    IPC分类号: C30B29/22 C01G41/00 B82Y30/00

    摘要: A process for preparing various morphology NTE compound ZrW0.5Mo1.5O8 comprising: preparing 0.4M Zr4+ solution, 0.2M W6+ solution and 0.6M Mo6+ solution with zirconyl nitrate, ammonium tungstate and ammo-nium molybdate separately, mixing them with the same volume and stirring until they are mixed well, adding 6-12M hydrochloric acid with the volume of 1/5-1/7 of the mixed solution, or adding 6-12M hydrochloric acid with the volume of 1/3-1/5 of the mixed solution and 0.2-0.4 wt % ammonium monoacid phosphate of all raw materials, or adding 9-18M sulfuric acid with the volume of 1/10-1/5 of the mixed solution, well mixing, transferring the mixed solution into the hydrothermal reactor, reacting at 150-180° C. for 8-25 hours, washing, drying and getting the precursor, heating the precursor at 480-500° C. for more than 5 hours and obtaining the product is provided.

    摘要翻译: 制备各种形态NTE化合物ZrW0.5Mo1.5O8的方法,包括:分别制备0.4M Zr4 +溶液,0.2M W6 +溶液和0.6M Mo6 +溶液,分别用硝酸锆铵,钨酸铵和钼酸铵,将它们与相同体积和 搅拌至充分混合,加入混合溶液体积为1 / 5-1 / 7的6-12M盐酸,或加入体积为1 / 3-1 / 5的6-12M盐酸 溶液和0.2-0.4重量%的所有原料磷酸一铵,或加入混合溶液体积为1 / 10-1 / 5的9-18M硫酸,充分混合,将混合溶液转移到水热反应器中, 在150-180℃下反应8-25小时,洗涤,干燥并得到前体,在480-500℃下加热前体超过5小时,得到产物。