摘要:
[Problems] To provide: a polypropylene resin composition which can produce an expansion-molded article showing excellent low-temperature impact properties even when expanded at an increased expansion rate; an expansion-molded article using the polypropylene resin composition, which has excellent low-temperature impact properties, is light in weight, and has good appearance; and a process for producing the expansion-molded article.[Solution] Using a polypropylene resin composition comprising 100 weight of a polypropylene resin and 1 to 4 parts by weight of a polyethylene wax having a viscosity average molecular weight of 2400 to 3400, an expansion-molded article which is expanded at an expansion rate of 1.5 to 3 times is produced by injection expansion molding by means of a gas counter pressure technique.
摘要:
A polypropylene resin composition which can produce an expansion-molded article showing excellent low-temperature impact properties even when expanded at an increased expansion rate; an expansion-molded article using the polypropylene resin composition, which has excellent low-temperature impact properties, is light in weight, and has good appearance; and a process for producing the expansion-molded article. Using a polypropylene resin composition comprising 100 weight of a polypropylene resin and 1 to 4 parts by weight of a polyethylene wax having a viscosity average molecular weight of 2400 to 3400, an expansion-molded article which is expanded at an expansion rate of 1.5 to 3 times is produced by injection expansion molding by means of a gas counter pressure technique.