Method for manufacturing a wide film, and wide film
    3.
    发明授权
    Method for manufacturing a wide film, and wide film 有权
    制造宽膜,宽膜的方法

    公开(公告)号:US09428624B2

    公开(公告)日:2016-08-30

    申请号:US13606236

    申请日:2012-09-07

    摘要: A method for manufacturing a wide film comprises a casting operation, a stretching operation, and a trimming operation. The casting operation is a process of casting a film using a wide casting belt including a central belt, a left belt having a right end formed integrally with a left end of the central belt through a left joint in a length direction of the central belt, and a right belt having a left end formed integrally with a right end of the central belt through a right joint in the length direction of the central belt. The stretching operation is a process of stretching a film stripped off from the wide casting belt using a tenter. The trimming operation is a process of trimming predetermined parts of left and right sides of the stretched film. In the trimming operation, mark parts by the left and right joints are also trimmed.

    摘要翻译: 制造宽膜的方法包括铸造操作,拉伸操作和修整操作。 铸造操作是使用宽的铸造带铸造膜的过程,该铸造带包括中心带,左侧带,其右端通过中心带的长度方向上的左接头与中心带的左端一体地形成, 以及右侧带,其左端通过中心带的长度方向上的右侧接头与中心带的右端一体地形成。 拉伸操作是使用拉幅机拉伸从宽流延带剥离的膜的过程。 修剪操作是修整拉伸膜的左侧和右侧的预定部分的过程。 在修剪操作中,还会修剪左右关节标记零件。

    Microporous polyolefin composite film with a thermally stable porous layer at high temperature
    6.
    发明授权
    Microporous polyolefin composite film with a thermally stable porous layer at high temperature 有权
    在高温下具有热稳定多孔层的微孔聚烯烃复合膜

    公开(公告)号:US08795826B2

    公开(公告)日:2014-08-05

    申请号:US12936416

    申请日:2009-04-08

    IPC分类号: B32B5/22

    摘要: Provided is a microporous polyolefin composite film with a thermally stable porous layer at high temperature, particularly, to the microporous polyolefin composite film in which the thermally stable porous layer at high temperature, which contains organic or inorganic particles and heat-resistant polymer having aromatic ring in main chain and also having a melting temperature or a glass transition temperature of 170 to 500° C., is formed on one surface or both surfaces of a polyolefin microporous film by a phase separation, wherein the composite film with the porous layer has a permeability of 1.5×10−5 to 20.0×10−5 Darcy, a meltdown temperature of 160 to 300° C., a MD/TD shrinkage of 1 to 40% at a temperature of 150° C. for 60 minutes.

    摘要翻译: 本发明提供一种在高温下具有热稳定性多孔层的微孔聚烯烃复合膜,特别是涉及含有有机或无机颗粒的热稳定多孔层和具有芳环的耐热聚合物的微孔聚烯烃复合膜 在聚烯烃微多孔膜的一个表面或两个表面上通过相分离形成熔融温度或玻璃化转变温度为170〜500℃,其中具有多孔层的复合膜具有 渗透率为1.5×10-5〜20.0×10-5达西,熔融温度为160〜300℃,MD / TD收缩率为1〜40%,温度为150℃60分钟。