公开(公告)号:US4646977A
公开(公告)日:1987-03-03
申请号:US613344
申请日:1984-05-23
申请人: Yoshinari Iwamura , Katsunori Okimoto , Toshio Teshima , Shinobu Miyahara , Shigetaka Uchida , Taizo Sera , Koichi Ozawa
发明人: Yoshinari Iwamura , Katsunori Okimoto , Toshio Teshima , Shinobu Miyahara , Shigetaka Uchida , Taizo Sera , Koichi Ozawa
摘要: A spray nozzle which has a nozzle main body and opening at one end in fluid communication with an inflow hole passing into the central portion of the nozzle main body. The inflow hole has a rounded orifice portion in fluid communication with an elongated discharge slot at an opposite end of the nozzle main body. Stirring channels extend along and are in fluid communication with the inflow hole. Each stirring channel has a cup-shaped end which is laterally adjacent the rounded orifice portion of the inflow hole. The cut-shaped portion of the stirring holes causes a reverse flow of mixed gas and liquid which passes down the stirring channels such that mixed gas and liquid passing through the inflow hole towards the elongated discharge slot is agitated and a uniform spray with fine droplets is jetted from the discharge slot.
摘要翻译: 一种喷嘴,其具有喷嘴主体,并且在一端开口,与通向喷嘴主体的中心部分的流入孔流体连通。 流入孔具有与喷嘴主体的相对端处的细长排出槽流体连通的圆形孔口部分。 搅拌通道沿着流入孔延伸并且与流入孔流体连通。 每个搅拌通道具有与流入孔的圆形孔部横向相邻的杯形端。 搅拌孔的切割部分引起通过搅拌通道的混合气体和液体的反向流动,从而搅拌通过流入孔的混合气体和液体朝向细长排出槽,并且具有细小液滴的均匀喷雾是 从排放槽喷出。
-
公开(公告)号:US4010792A
公开(公告)日:1977-03-08
申请号:US627065
申请日:1975-10-30
申请人: Moriyuki Ishiguro , Shinobu Miyahara , Isao Sugawara , Masayuki Hanmyo , Shigetaka Uchida , Hideo Uchibori , Shigeki Komori
发明人: Moriyuki Ishiguro , Shinobu Miyahara , Isao Sugawara , Masayuki Hanmyo , Shigetaka Uchida , Hideo Uchibori , Shigeki Komori
IPC分类号: B22D11/128 , B22D11/12
CPC分类号: B22D11/1206
摘要: In continuously casting steel, at least two pairs of reduction rolls are arranged near the crater top where the solidification of the molten steel in the cast strand is completed, said reduction rolls having a roll pitch of 200 to 420mm and giving a draft per pair of 0.1 to 2.0%, and said cast strand is reduced near the to of said crater, whereby the inner quality of said cast strand is remarkably improved.
摘要翻译: 在连续铸造钢中,至少两对还原辊布置在铸造线中的钢水凝固完成的火山口顶部附近,所述还原辊的辊间距为200至420mm,并且每一对 0.1-2.0%,并且所述铸线在所述火山口附近减小,由此所述铸造线的内部质量显着提高。
-
公开(公告)号:US5033534A
公开(公告)日:1991-07-23
申请号:US487758
申请日:1990-03-02
申请人: Mikio Suzuki , Toru Kitagawa , Shinobu Miyahara , Akio Nagamune , Yoshiyuki Kanao , Norio Ao , Hironori Yamamoto
发明人: Mikio Suzuki , Toru Kitagawa , Shinobu Miyahara , Akio Nagamune , Yoshiyuki Kanao , Norio Ao , Hironori Yamamoto
IPC分类号: B22D11/115
CPC分类号: B22D11/115
摘要: A method for continuous casting of steel comprises charging molten steel from a tundish into a mold through exit ports of an immersion nozzle, introducing a magnetic field vertically to a flow of the molten steel from the exit ports by the use of at least a pair of direct current magnets which are arranged on the outer side of copper plates on the wide side of the mold, the immersion nozzle being placed between the direct current magnets and polarities of magnetisms on the top side of the magnets being the same, and casting the molten steel at a predetermined casting rate. One magnetic pole of the direct current magnet is positioned at an upper end of copper plate on the wide side of the mold and the other magnetic pole being positioned at lower than the exit port of the immersion nozzle and on the outer side of copper plate on the wide side of the mold. The immersion nozzle has two exit ports, each of which has an angle of 15.degree. to 45.degree. downward. The direct current magnetic field is controlled within the range of 1000 to 4000 gauss.
-
公开(公告)号:US4134440A
公开(公告)日:1979-01-16
申请号:US751618
申请日:1976-12-16
申请人: Takaho Kawawa , Hideki Sato , Shinobu Miyahara
发明人: Takaho Kawawa , Hideki Sato , Shinobu Miyahara
CPC分类号: B22D11/225 , B22D11/207
摘要: In continuously casting molten steel at least a pair of rolls is disposed near the leading end of the crater at which solidification of the molten steel in the cast piece completes so as to roll the cast piece at a reduction rate of from 0.1 to 2.0%. The variation in the thickness of the cast piece is detected and compared with a definite reference value for controlling the drawing speed and or the quantity of the secondary cooling water.
摘要翻译: 在连续铸造钢水中,至少一对辊设置在火山口的前端附近,铸钢件中的钢水的凝固完成,从而以0.1-2.0%的压下率滚动铸件。 检测铸件厚度的变化,并将其与用于控制二次冷却水的拉拔速度和数量的确定参考值进行比较。
-
-
-