公开(公告)号:US5717004A
公开(公告)日:1998-02-10
申请号:US751476
申请日:1996-11-18
CPC分类号: C08F2/46 , B01J19/123 , C03C17/32 , C09D4/00
摘要: The composition of the present invention is curable by active energy ray. It is a mixture including a coupling agent, an active energy ray-curable compound and water. A glass article will show improved mechanical strength if it is coated with the composition of the present invention and irradiated with active energy ray to cure the coating.
摘要翻译: 本发明的组合物可通过活性能量射线固化。 它是一种包括偶联剂,活性能量射线固化性化合物和水的混合物。 如果涂覆本发明的组合物并用活性能量射线照射以固化涂层,玻璃制品将显示出改进的机械强度。
-
公开(公告)号:US5889074A
公开(公告)日:1999-03-30
申请号:US951633
申请日:1997-10-16
CPC分类号: C08F2/46 , B01J19/123 , C03C17/32 , C09D4/00
摘要: A method for improving mechanical strength of a glass article includes coating an active energy ray-curable composition of a silane coupling agent, a curable compound and water on the glass article, and then curing with irradiated active energy ray.
摘要翻译: 提高玻璃制品的机械强度的方法包括在玻璃制品上涂布硅烷偶联剂,固化性化合物和水的活性能量射线固化性组合物,然后用照射的活性能量光线固化。
-