公开(公告)号:WO2008148986A2
公开(公告)日:2008-12-11
申请号:PCT/FR2008050782
申请日:2008-05-02
Applicant: CT REGIONAL D INNOVATION ET DE , AIR LIQUIDE , MAZET THIERRY , JULLIARD FRANCK , RIDLOVA MARTINA , DULCY JACKY , GANTOIS MICHEL
Inventor: MAZET THIERRY , JULLIARD FRANCK , RIDLOVA MARTINA , DULCY JACKY , GANTOIS MICHEL
CPC classification number: B23K1/008 , B22F2998/00 , B23K35/286 , B23K35/362 , B23K35/38 , B23K2203/10 , C22C21/02 , C22C1/0416 , C22C1/0491
Abstract: The present invention relates to an aluminium brazing method conducted in an atmospheric-pressure furnace, which is characterized by the implementation of the following operational conditions: i) the filler alloy used is an alloy obtained by mechanical synthesis, comprising aluminium, silicon, nickel and optionally magnesium or other alloying elements, such as copper, zinc, silver, chromium and titanium; j) the oxygen content in the furnace is less than a few ppm, preferably less than 1 ppm and that the dew point in the furnace is below -30°C, preferably below -40°C and even more preferably still below -45°C.
Abstract translation: 本发明涉及一种在常压炉中进行的铝钎焊方法,其特征在于实施以下操作条件:i)所用的填料合金是通过机械合成获得的合金,包括铝,硅,镍和 任选的镁或其它合金元素,例如铜,锌,银,铬和钛; j)炉中的氧含量小于几ppm,优选小于1ppm,并且炉中的露点低于-30℃,优选低于-40℃,甚至更优选低于-45℃ C。