Abstract: A process for producing a carbon material comprising heating a compound represented by the formula (1): wherein R represents a hydrogen atom or a C1-C12 hydrocarbon group which may be substituted with at least one selected from the group consisting of a hydroxyl group, a C1-C6 alkoxy group, a C6-C20 aryloxy group, a sulfonyl group, a nitro group, a C1-C6 thioalkyl group, a cyano group, a carboxyl group, an amino group, a C2-C20 acylamino group and a halogen atom, R' represents a hydrogen atom or a methyl group, and n represents an integer of 3 to 7, at 800 to 3,000oC under an inert gas atmosphere.
Abstract translation: 一种制备碳材料的方法,该方法包括加热由式(1)表示的化合物:其中R表示氢原子或可被至少一个选自下列的基团取代的C1-C12烃基:羟基, C 1 -C 6烷氧基,C 6 -C 20芳氧基,磺酰基,硝基,C 1 -C 6硫代烷基,氰基,羧基,氨基,C 2 -C 20酰氨基和卤素 原子,R'表示氢原子或甲基,n表示3〜7的整数,在惰性气体气氛下,在800〜3000℃下进行。
-
公开(公告)号:WO2009101947A3
公开(公告)日:2009-08-20
申请号:PCT/JP2009/052250
申请日:2009-02-04
Applicant: SUMITOMO CHEMICAL COMPANY, LIMITED , SUZUKI, Junji , KIKUCHI, Taketoshi
Inventor: SUZUKI, Junji , KIKUCHI, Taketoshi
Abstract: A process for producing a carbon material comprising the following steps (A) and (B): Step (A): a step of reacting a compound represented by the formula (1): wherein R represents a hydrogen atom etc., R' represents a hydrogen atom etc., and n represents 3, 5 or 7, with an aldehyde compound to obtain a polymer, Step (B): a step of heating the polymer obtained in Step (A) at 600 to 3000 o C under an inert gas atmosphere.
-
公开(公告)号:WO2009101947A2
公开(公告)日:2009-08-20
申请号:PCT/JP2009052250
申请日:2009-02-04
Applicant: SUMITOMO CHEMICAL CO , SUZUKI JUNJI , KIKUCHI TAKETOSHI
Inventor: SUZUKI JUNJI , KIKUCHI TAKETOSHI
CPC classification number: H01M4/587 , C01B32/05 , C01P2006/12 , C08G8/20 , H01G11/32 , H01G11/42 , H01G11/48 , H01M4/133 , H01M10/0525 , Y02E60/13
Abstract: A process for producing a carbon material comprising the following steps (A) and (B): Step (A): a step of reacting a compound represented by the formula (1): wherein R represents a hydrogen atom etc., R' represents a hydrogen atom etc., and n represents 3, 5 or 7, with an aldehyde compound to obtain a polymer, Step (B): a step of heating the polymer obtained in Step (A) at 600 to 3000oC under an inert gas atmosphere.
Abstract translation: 一种碳材料的制造方法,其特征在于,包括以下工序(A)和工序(B):工序(A):使式(1)所示的化合物:其中,R表示氢原子等,R'表示 (B):将工序(A)中得到的聚合物在惰性气体气氛下在600〜3000℃加热的工序(a),将氢原子等与n表示3,5或7的化合物与醛化合物反应而得到聚合物。 。
-
公开(公告)号:WO2009078371A2
公开(公告)日:2009-06-25
申请号:PCT/JP2008/072721
申请日:2008-12-08
Applicant: SUMITOMO CHEMICAL COMPANY, LIMITED , KURAKANE, Kosuke , KIKUCHI, Taketoshi , TAMATO, Toyomochi
Inventor: KURAKANE, Kosuke , KIKUCHI, Taketoshi , TAMATO, Toyomochi
Abstract: A process for producing a carbon material comprising heating a compound represented by the formula (1): wherein R represents a hydrogen atom or a C1-C12 hydrocarbon group which may be substituted with at least one selected from the group consisting of a hydroxyl group, a C1-C6 alkoxy group, a C6-C20 aryloxy group, a sulfonyl group, a nitro group, a C1-C6 thioalkyl group, a cyano group, a carboxyl group, an amino group, a C2-C20 acylamino group and a halogen atom, R' represents a hydrogen atom or a methyl group, and n represents an integer of 3 to 7, at 800 to 3,000oC under an inert gas atmosphere.
Abstract translation: 一种制备碳材料的方法,包括加热式(1)表示的化合物:其中R表示氢原子或可被至少一个选自羟基, C1-C6烷氧基,C6-C20芳氧基,磺酰基,硝基,C1-C6硫代烷基,氰基,羧基,氨基,C2-C20酰氨基和卤素 在惰性气体气氛下,在800〜3000℃下,R'表示氢原子或甲基,n表示3〜7的整数。
-
-
-