公开(公告)号:WO2008132497A1
公开(公告)日:2008-11-06
申请号:PCT/GB2008/050255
申请日:2008-04-11
Applicant: BPB LTD , BIGUENET, Cedric , O'KEEFE, Sam
Inventor: BIGUENET, Cedric , O'KEEFE, Sam
IPC: C04B28/14 , C04B11/024
CPC classification number: C04B28/147 , C04B11/024 , C04B2103/302 , C04B2201/50 , C04B20/0048 , C04B22/147 , C04B22/148 , C04B38/10 , C04B11/036
Abstract: A gypsum stucco composition comprising the following components finely divided; calcium sulphate hemihydrate in calcined solid beta crystalline form; and in intimate mixture with said finely divided calcium sulphate hemihydrate and mixed therewith no later than calcination to form the hemihydrate, a sulphate salt comprising at least one of ammonium sulphate and aluminium sulphate, in an amount such that when the stucco composition is mixed with water and allowed to set, the resulting set plaster has increased compressive strength, flexural strength and/or E-modulus compared to a set plaster produced from said finely divided calcium sulphate hemihydrate containing no said sulphate salt.
Abstract translation: 一种石膏灰泥组合物,其包含细分的以下组分; 煅烧固体β晶型的硫酸钙半水合物; 并且与所述细碎的硫酸钙半水合物紧密地混合并且不迟于煅烧混合以形成半水合物,包含硫酸铵和硫酸铝中的至少一种的硫酸盐,其量使得当灰泥组合物与水混合时 并且允许固化,与由不含所述硫酸盐的所述细碎的硫酸钙半水合物制成的固定石膏相比,所得到的固化石膏具有增加的抗压强度,弯曲强度和/或E模量。
-
公开(公告)号:WO2007045923A3
公开(公告)日:2007-08-02
申请号:PCT/GB2006050332
申请日:2006-10-17
Applicant: BPB PLC , O'KEEFE SAM , SAHAY PARNIKA
Inventor: O'KEEFE SAM , SAHAY PARNIKA
IPC: C04B28/14 , B01F11/02 , C04B40/00 , C04B103/10
CPC classification number: C04B28/14 , B01F11/0258 , C04B40/0021 , C04B2111/0062 , C04B22/147 , C04B40/0028 , C04B40/0227 , C04B2103/10
Abstract: A method of accelerating the setting reaction of calcium sulphate hemihydrafce and water comprises the steps of mixing water and calcium sulphate hemihydrate to produce a slurry adding an accelerator to said mixture applying ultrasonic energy to said mixture. Application of ultrasound to the plaster slurry accelerates crystallization and thus reduces the setting time. A further benefit is reduced density of the wall boards.
Abstract translation: 加速硫酸钙半水合物和水的凝固反应的方法包括将水和硫酸钙半水合物混合以产生向所述混合物中加入促进剂的浆料,向所述混合物中施加超声波能量。 将超声波应用于石膏浆加速结晶,从而减少凝固时间。 另一个好处是减少墙板的密度。
-
公开(公告)号:WO2007045923A2
公开(公告)日:2007-04-26
申请号:PCT/GB2006/050332
申请日:2006-10-17
Applicant: BPB PLC , O'KEEFE, Sam , SAHAY, Parnika
Inventor: O'KEEFE, Sam , SAHAY, Parnika
CPC classification number: C04B28/14 , B01F11/0258 , C04B40/0021 , C04B2111/0062 , C04B22/147 , C04B40/0028 , C04B40/0227 , C04B2103/10
Abstract: A method of accelerating the setting reaction of calcium sulphate hemihydrate and water comprises the steps of mixing water and calcium sulphate hemihydrate to produce a slurry adding an accelerator to said mixture applying ultrasonic energy to said mixture.
Abstract translation: 加速硫酸钙半水合物和水的凝固反应的方法包括以下步骤:将水和硫酸钙半水合物混合以产生向所述混合物中加入促进剂的浆料,向所述混合物中施加超声波能量。
-
-