Abstract:
Heterophasic polypropylene composition with improved impact strength/stiffness balance and with high flowability, reduced emissions and low shrinkage, and its use.
Abstract:
The invention relates to a propylene homopolymer or copolymer having a comonomer in the copolymer selected from ethylene, C4-C20-alpha olefin, said propylene homopolymer or copolymer being free of phthalic compound. It further relates to a long-chain branched propylene homopolymer or copolymer (b-PP) having a comonomer in the copolymer selected from ethylene, C4-C20-alpha olefins, said long-chain branched propylene homopolymer or copolymer (b-PP) being free of phthalic compound. As well as their production processes and uses.
Abstract:
The invention relates to a propylene homopolymer or copolymer having a comonomer in the copolymer selected from ethylene, C4-C20-alpha olefin, said propylene homopolymer or copolymer being free of phthalic compound. It further relates to a long-chain branched propylene homopolymer or copolymer (b-PP) having a comonomer in the copolymer selected from ethylene, C4-C20-alpha olefins, said long-chain branched propylene homopolymer or copolymer (b-PP) being free of phthalic compound. As well as their production processes and uses.
Abstract:
Extrusion blown film comprising a polypropylene composition, said polypropylene composition comprises a random propylene copolymer, a high melt strength polypropylene, and optionally a clarifier, wherein ° the random propylene copolymer comprises units derived from propylene and at least another C2 to C20 a-olefm. ° the high melt strength polypropylene has a branching index g' of less than 1.0. ° the clarifier comprises at least one a-nucleating agent, and wherein further ° the branching index g' of the random propylene copolymer is higher than the branching index g' of the high melt strength polypropylene, ° the extrusion melt blown film and/or the polypropylene composition, (i) fulfill(s) the equation (I) Tm-Tc = 30 wherein Tm is the melting temperature [°C] making up more than 50% of the total melting enthalpy Hm of the extrusion melt blown film or of the polypropylene composition measured by DSC according to ISO 11357-3; Tc is the crystallization temperature [°C] of the extrusion melt blown film or of the polypropylene composition measured by DSC according to ISO 11357-3; and/or (ii) has (have) a melt flow rate MFR2 (230 °C) measured according to ISO 1133 of 1.0 to 5.5 g/10min.