COMPOSITIONS COMPRISING A PROPYLENE-BASED ELASTOMER AND A POLYALPHAOLEFIN, METHODS OF MAKING THE SAME, AND ARTICLES MADE THEREFROM
    1.
    发明申请
    COMPOSITIONS COMPRISING A PROPYLENE-BASED ELASTOMER AND A POLYALPHAOLEFIN, METHODS OF MAKING THE SAME, AND ARTICLES MADE THEREFROM 审中-公开
    包含基于丙烯的弹性体和聚对苯二甲酸乙二醇酯的组合物,其制备方法及其制备方法

    公开(公告)号:WO2013158239A1

    公开(公告)日:2013-10-24

    申请号:PCT/US2013/029876

    申请日:2013-03-08

    Abstract: The present disclosure is directed to compositions comprising: (a) a propylene-based elastomer, comprising at least about 60 wt% propylene-derived units and about 5 to about 25 wt% ethylene-derived units, based on total weight of the propylene-based elastomer, wherein the propylene-based elastomer has a heat of fusion of less than about 80 J/g; and (b) a polyalphaolefin. Such compositions have at least one of the following properties: (a) a hardness of about 25 to about 67 shore A (ASTM D2240); (b) a glass transition temperature of about -35°C to about -65°C (ASTM D3418-08, 10°C/min); and (c) an impact resistance at a temperature no lower than about -40°C (ASTM D3763).

    Abstract translation: 本公开涉及包含以下组分的组合物:(a)丙烯类弹性体,其包含至少约60重量%的丙烯衍生单元和约5至约25重量%的来自乙烯的单元,基于丙烯 - 其中所述丙烯类弹性体具有小于约80J / g的熔化热; 和(b)聚α-烯烃。 这样的组合物具有以下特性中的至少一种:(a)约25至约67肖氏硬度A(ASTM D2240); (b)约-35℃至约-65℃的玻璃化转变温度(ASTM D3418-08,10℃/ min); 和(c)在不低于约-40℃的温度下的耐冲击性(ASTM D3763)。

    POLYMER BLEND, METHOD FOR MAKING THE SAME AND ROOFING MEMBRANE CONTAINING THE SAME
    7.
    发明申请
    POLYMER BLEND, METHOD FOR MAKING THE SAME AND ROOFING MEMBRANE CONTAINING THE SAME 审中-公开
    聚合物混合物,制备聚合物混合物的方法和包含其的屋面膜

    公开(公告)号:WO2017105550A1

    公开(公告)日:2017-06-22

    申请号:PCT/US2016/043057

    申请日:2016-07-20

    CPC classification number: C08L23/12 C08L23/16

    Abstract: A polymer blend comprising 10 to 90 parts by weight of a propylene-based polymer component having a weight average molecular weight of at least 200 kg⋅mol -1 ; and 20 to 80 parts by weight of a propylene-based elastomer component comprising structural units derived from propylene and at least one of ethylene and C4-C12 alpha-olefins having a weight average molecular weight in the range from 5 to 50 kg⋅mol -1 , method for making a membrane comprising the same and roofing membrane comprising the same. The polymer blend is particularly suitable for making roofing membrane due to advantageous elastic modulus in broad temperature ranges.

    Abstract translation: 包含10至90重量份的重均分子量为至少200kg·mol -1的基于丙烯的聚合物组分的聚合物共混物; 和20至80重量份的基于丙烯的弹性体组分,所述基于丙烯的弹性体组分包含衍生自丙烯的结构单元和乙烯和重均分子量为5至50kg·mol -1的C4-C12α-烯烃中的至少一种< 制备包含该膜的膜和包含该膜的屋顶膜的方法。 由于在宽温度范围内有利的弹性模量,聚合物共混物特别适用于制造屋面膜。