CPC classification number: C03C8/24 , B01D65/003 , B01D71/024 , C03C10/0018 , C04B35/6264 , C04B35/632 , C04B35/6342 , C04B35/638 , C04B37/005 , C04B37/025 , C04B2235/6562 , C04B2235/6565 , C04B2237/10 , C04B2237/348 , C04B2237/40 , C04B2237/401 , C04B2237/60 , C04B2237/708 , C04B2237/765 , H01M8/0282 , H01M8/0286 , Y10T403/477
Abstract: An improved method of sealing a ceramic part to a solid part made of ceramic, metal, cermet or a ceramic coated metal is provided. The improved method includes placing a bond agent comprising an Al 2 O 3 and SiO 2 based glass- ceramic material and organic binder material on adjoining surfaces of the ceramic part and the solid part. The assembly is heated to a first target temperature that removes or dissolves the organic binder material from the bond agent and the assembly is subjected to a second induction heating step at a temperature ramp rate of between about 100°C and 200°C per minute to temperatures where the glass- ceramic material flows and wets the interface between adjoining surfaces. The assembly is rapidly cooled at a cooling rate of about 140°C per minute or more to induce nucleation and re-crystallization of the glass-ceramic material to form a dense, durable and gas-tight seal.
Abstract translation: 提供了一种将陶瓷部件密封到由陶瓷,金属,金属陶瓷或陶瓷涂覆的金属制成的实心部件的改进方法。 改进的方法包括将包含Al 2 O 3和SiO 2的玻璃 - 陶瓷材料和有机粘合剂材料的粘合剂放置在陶瓷部分和固体部分的相邻表面上。 将组件加热到第一目标温度,其从粘合剂中除去或溶解有机粘合剂材料,并且该组件以约100℃至200℃/分钟的温度升温速率进行第二感应加热步骤, 玻璃陶瓷材料流动并润湿相邻表面之间的界面的温度。 该组件以约140℃/分钟或更高的冷却速度快速冷却,以引起玻璃 - 陶瓷材料的成核和重结晶,从而形成密实,耐用且气密的密封。