Abstract:
Provided is a suspension comprising liquid droplets dispersed in an aqueous medium, wherein said droplets comprise (a) one or more water-insoluble compounds, and (b) a vinyl polyelectrolyte (PED) having a polarity, and wherein said aqueous medium comprises a polyelectrolyte (PEW) having a polarity that is opposite to the polarity of said polyelectrolyte (PED). Also provided are a method of making such a suspension and a method using such a suspension in a process of suspension polymerization.
Abstract:
Provided is vinyl aromatic resin comprising benzyl alcohol groups, benzyl ether groups, and methylene bridge groups, wherein the mole ratio of the benzyl ether groups to the methylene bridge groups is from 0.002:1 to 0.1:1, wherein the vinyl aromatic resin either has no amine groups or else has amine groups in a mole ratio of the sum of all amine groups to aromatic rings of 0.1:1 or lower.
Abstract:
Provided is a method of suspension polymerization comprising (i) providing a suspension of liquid droplets in an aqueous medium, wherein said droplets comprise (a) one or more water-insoluble vinyl monomers, and (b) a polyelectrolyte (PED) having a polarity, (c) one or more initiators, and wherein said aqueous medium comprises a polyelectrolyte (PEW) having a polarity that is opposite to the polarity of said polyelectrolyte (PED), (ii) polymerizing said vinyl monomer or allowing said vinyl monomer to polymerize.
Abstract:
A thin film composite polyamide membrane having a porous support and a thin film polyamide layer comprising a reaction product of m-phenylene diamine (mPD) and trimesoyl chloride (TMC), characterized by the thin film polyamide layer having a critical strain value of less than 10%. In another embodiment, the thin film polyamide layer has a modulus of greater than 0.75 (GPa). In yet another embodiment, the thin film polyamide layer has an equilibrium swelling value of at least 45%. In another embodiment, the thin film polyamide layer has a thickness of at least 230 nm.
Abstract:
A method for making a composite polyamide membrane including the steps of applying a polyfunctional amine monomer and polyfunctional acid halide monomer to a surface of the porous support and interfacially polymerizing the monomers to form a thin film polyamide layer, wherein the method is includes at least one of the following steps: i) conducting the interfacial polymerization in the presence of an additional monomer comprising an aromatic moiety at least one carboxylic acid functional group or salt thereof and a single amine-reactive functional group; and/or ii) applying such a monomer to the thin film polyamide layer. Many additional embodiments are described including applications for such membranes.
Abstract:
A thin film composite polyamide membrane comprising a porous support and a thin film polyamide layer characterized by possessing an azo (-N=N-) content of from 0.75% to 0.95%, as measured by pyrolysis gas chromatography.
Abstract:
A thin film composite polyamide membrane including a porous support and a thin film polyamide layer which is a reaction product of m-phenylene diamine (mPD) and trimesoyl chloride (TMC), wherein the membrane is characterized by the thin film polyamide layer having a dissociated carboxylic acid content of at least 0.18 moles/kg at pH 9.5, and wherein pyrolysis of the thin film polyamide layer at 650C results in a ratio of responses from a flame ionization detector for fragments produced at 212 m/z and 237 m/z of less than 2.8.
Abstract:
A method for preparing a high purity (e.g. greater than 70 wt. %) mono-hydrolyzed acyl halide compound as a precipitate from solution comprising the steps of preparing a solution comprising: i) at least 80 v/v% of a hydrocarbon solvent, ii) water at a molar concentration greater than its solubility limit within the solvent but less that its solubility limit in solution, iii) a tri-hydrocarbyl phosphate compound, and iv) a polyfunctional acyl halide compound at molar ratio to both water and the tri-hydrocarbyl phosphate compound of at least 1:1.
Abstract:
A thin film composite polyamide membrane comprising a porous support and a thin film polyamide layer characterized by possessing: i) an azo (-N=N-) content of from 0.40% to 1.00%, as measured by pyrolysis gas chromatography; and ii) a dissociated carboxylate content of at least 0.40 mol/kg as measured by RBS at pH 9.5.
Abstract:
A method for making a composite polyamide membrane including a porous support and a thin film polyamide layer including the steps of applying a polyfunctional amine monomer and a combination amine-reactive compounds to a surface of the porous support and reacting the constituents to form a thin film polyamide layer, wherein the amine-reactive compounds include: i) a polyfunctional amine-reactive monomer including two to three amine-reactive moieties selected from acyl halide, sulfonyl halide and anhydride, ii) a polyfunctional amine-reactive monomer including at least four amine-reactive moieties selected from acyl halide, sulfonyl halide and anhydride, and iii) an acid compound including at least on carboxylic acid moiety or salt thereof and at least one amine-reactive moiety selected from acyl halide and sulfonyl halide.