POLYMER STABILIZERS FOR BITUMINOUS EMULSIONS

    公开(公告)号:EP3227391B1

    公开(公告)日:2018-07-11

    申请号:EP15807832.9

    申请日:2015-12-02

    IPC分类号: C08L95/00

    摘要: A mineral-compatible cationic emulsion composition with polymer stabilizers, and methods for utilizing same in paving and other applications is disclosed. In one aspect, a bitumen-in-water emulsion composition includes at least one bitumen material, at least one polymer stabilizer, at least one emulsifier, and water, where the emulsifier is a cationic surfactant, an amphoteric surfactant, or a mixture of both, and the polymer stabilizer is a natural or synthetic cationic polymer consisting of alkylene polyamines, alkyl polyamines, polyquaternary polymers, polyvinylamine, polyvinylimidazoline, polyester polyquaternary polymers, polyether polyquaternary polymers, or mixtures thereof. The inclusion of polymer stabilizer in the cationic emulsion increases the stability of the emulsion and increases the compatibility of the cationic emulsion with negatively charged minerals.

    Process of preparing polyamine-epihalohydrin resins with reduced byproduct content
    60.
    发明公开
    Process of preparing polyamine-epihalohydrin resins with reduced byproduct content 有权
    制备副产物含量降低的聚胺 - 表卤代醇树脂的方法

    公开(公告)号:EP1770109A3

    公开(公告)日:2007-10-03

    申请号:EP07000112.8

    申请日:2000-06-12

    摘要: A process for rendering a polyamine-epihalohydrin resin storable stable, comprising: treating a composition containing a polyamine-epihalohydrin resin which includes CPD-forming species with at least one acidic agent, wherein the pH during treatment is about 1.1 or less; the time is for at least about 2 hours to at least about 24 hours, and the temperature is at least about 30 °C to at least about 90 °C, wherein the temperature range is combined with the time period range in an inverse relationship, to at least one of inhibit, reduce and remove the CPD-forming species to obtain a gelation storage stable reduced CPD-forming resin so that the composition containing the reduced CPD-forming polyamine-epihalohydrin resin, when stored at pH 1 for 24 hours at 50 °C and measured at 24 hours, produces less than about 500 ppm dry basis of CPD.

    摘要翻译: 一种使聚胺 - 表卤代醇树脂储存稳定的方法,包括:用至少一种酸性试剂处理含有包含CPD形成物质的聚胺 - 表卤代醇树脂的组合物,其中处理期间的pH值为约1.1或更小; 时间为至少约2小时至至少约24小时,并且温度为至少约30℃至至少约90℃,其中温度范围与时间范围以相反的关系相结合, 以抑制,还原和去除形成CPD的物质中的至少一种,以获得凝胶储存稳定减少的CPD形成树脂,使得当在pH 1下储存24小时时,含有形成CPD的减少的多胺 - 表卤代醇树脂的组合物 50°C,并在24小时测量,产生的CPD的干基数小于约500 ppm。