METHOD FOR MANUFACTURING ORGANIC SOLAR CELL
    71.
    发明公开
    METHOD FOR MANUFACTURING ORGANIC SOLAR CELL 审中-公开
    方法用于生产有机太阳能电池

    公开(公告)号:EP2798681A1

    公开(公告)日:2014-11-05

    申请号:EP12861743.8

    申请日:2012-05-31

    IPC分类号: H01L51/48

    摘要: A method of manufacturing an organic solar cell is provided. According to the exemplary embodiments of the present invention, a laminate section can be easily removed from a substrate by causing a cleaning unit to move up and down above the substrate or to move forward and backward in a reciprocating manner in the width direction of the substrate. Furthermore, when a contact member is detachably connected to the cleaning unit, the contact member that has been contaminated with a laminate material can be separated from the cleaning unit and easily washed. Also, the laminate section can be removed by spraying a solvent through a discharging unit to dissolve the laminate section, and suctioning the laminate section through a suctioning unit. In this case, the laminate section can be easily removed from the substrate by dissolving the laminate section with the solvent.

    ARAMID FABRIC AND AIRBAG FOR VEHICLE INCLUDING SAME
    72.
    发明公开
    ARAMID FABRIC AND AIRBAG FOR VEHICLE INCLUDING SAME 有权
    阿拉伯联合酋长国安全资格FÜREIN FAHRZEUG DAMIT

    公开(公告)号:EP2796600A1

    公开(公告)日:2014-10-29

    申请号:EP12858851.4

    申请日:2012-12-21

    摘要: This invention relates to an aramid fabric and an airbag for a vehicle including the same, and more specifically, to an aramid fabric and an airbag for a vehicle including the same, wherein the aramid fabric can endure high levels of impact force and can exhibit superior air sealing performance, dimensional stability and packing property, and can thus be adapted for use in an external airbag for a vehicle. The aramid fabric includes an aramid fabric layer including an aramid yarn having a fineness of 300 to 1000 denier; and a rubber coating layer formed on the aramid fabric layer, wherein the strength-elongation index (TI wa ) in a warp direction of the fabric as defined by a predetermined equation is 2.8 to 4.8, and the coating amount of the rubber coating layer is 20 to 100 g/m 2 .

    摘要翻译: 本发明涉及一种芳族聚酰胺织物和一种包括该芳族聚酰胺织物的车辆用安全气囊,更具体地,涉及一种芳族聚酰胺织物和包括该芳族聚酰胺织物和用于车辆的气囊,其中芳族聚酰胺织物可以承受高水平的冲击力,并且可以表现出优异的 空气密封性能,尺寸稳定性和包装性,因此可以适用于用于车辆的外部气囊。 芳族聚酰胺织物包括芳族聚酰胺织物层,其包括细度为300至1000旦尼尔的芳族聚酰胺纱线; 以及形成在所述芳族聚酰胺织物层上的橡胶涂层,其中由规定的方程式定义的织物经纱方向的强度 - 伸长率(TI wa)为2.8〜4.8,橡胶被覆层的涂布量为 20〜100g / m 2。

    METHOD FOR MANUFACTURING POLY(ETHYLENETEREPHTHALATE) DRAWN FIBER, POLY(ETHYLENETEREPHTHALATE) DRAWN FIBER AND TIRE-CORD
    74.
    发明公开
    METHOD FOR MANUFACTURING POLY(ETHYLENETEREPHTHALATE) DRAWN FIBER, POLY(ETHYLENETEREPHTHALATE) DRAWN FIBER AND TIRE-CORD 审中-公开
    制造方法DRAWN聚(对苯二甲酸乙二醇酯)纤维DRAWN聚(对苯二甲酸乙二醇酯)纤维轮胎帘线,并且

    公开(公告)号:EP2761068A2

    公开(公告)日:2014-08-06

    申请号:EP12837107.7

    申请日:2012-09-25

    IPC分类号: D02J1/22 D01D5/08 D02G3/48

    摘要: The present invention relates to a method for manufacturing a drawn fiber, which is able to manufacture a poly(ethylene terephthalate) drawn fiber showing superior strength and dimensional stability and having a high fineness of 2000 denier or more without breakage or reduction in physical properties during the manufacturing process, and a poly(ethylene terephthalate) drawn fiber and a tire-cord obtained therefrom. The method for manufacturing a poly(ethylene terephthalate) drawn fiber comprises the steps of adding 0.1 to 2.0 wt% of a polyamide-based resin to a polymer including 90 mol% or more of poly(ethylene terephthalate) and having an intrinsic viscosity of 0.8 to 1.5; melt-spinning the polyamide-based resin-added polymer mixture through a spinneret at a speed of 2500 to 4000 m/min in a three- or four-ply spinning manner so as to produce an undrawn fiber having a fineness of 2000 denier or more; and drawing the undrawn fiber with a drawing ratio of 1.4 to 2.4.

    HYBRID FIBER AND METHOD FOR PRODUCING SAME
    79.
    发明公开
    HYBRID FIBER AND METHOD FOR PRODUCING SAME 审中-公开
    HYBRIDFASER UND HERSTELLUNGSVERFAHRENDAFÜR

    公开(公告)号:EP2617883A2

    公开(公告)日:2013-07-24

    申请号:EP11825387.1

    申请日:2011-09-09

    IPC分类号: D02G3/04 D02G3/26 D02G3/40

    摘要: The present disclosure relates to a hybrid fiber fabricated with a low production cost while having excellent mechanical properties, as well as a method for fabricating the same. The disclosed hybrid fiber includes; a first filament, and a second filament different from the first filament, wherein a strength-strain curve of the hybrid fiber measured according to ASTM D 885 has at least one peak, provided that, if the strength-strain curve has at least two or more peaks, a difference in strain between a first peak having the lowest strain and a second peak having the highest strain, among the above two or more peaks, is 3% or less.

    摘要翻译: 本公开内容涉及以低成本制造而具有优异的机械性能的混合纤维及其制造方法。 所公开的混合光纤包括: 第一丝和不同于第一丝的第二丝,其中根据ASTM D 885测量的复合纤维的强度 - 应变曲线具有至少一个峰,条件是如果强度 - 应变曲线具有至少两个或更多个 在上述两个以上的峰中,具有最低应变的第一峰与具有最高应变的第二峰之间的应变差为3%以下。