Abstract:
The present invention relates to compositions comprising (i) at least one molding compound comprising the components A and B as component (I), where A) means a graft copolymer as component A, and B) means a thermoplastic copolymer as component B; and (ii) at least one cyclohexane polycarbolic acid derivate of the formula (I); as component (II) where R 1 stands for C 1 -C 10 -alkyl or C 3 -C 8 -cycloalkyl, m stands for 0, 1, 2, or 3, n stands for 2, 3, or 4, and R stands for hydrogen or C 1 -C 30 -alkyl; or the group -(COOR) n forms an anhydride of the formula (II), wherein, according to the invention, the component (I) comprises 11 to 19.9% by weight of component A and 80.1 to 89% by weight of component B, wherein each % by weight is based on the sum of components A and B and together adds up to 100% by weight. The invention further relates to a method for producing the composition according to the invention, to the use of the composition according to the invention for producing molded parts, films, foams or fibers, and to molded parts, films, foams or fibers comprising the composition according to the invention.
Abstract:
A mixture comprising a) 5 to 95 wt.-% of a copolymer A that contains one or more copolymer blocks (B/S) A , each made of 65 to 95 wt.-% of vinyl aromatic monomers and 5 to 35 wt.-% dienes and having a glass transition temperature Tg A in the range of 40° to 90°C, b) 5 to 95 wt.-% of a block copolymer B containing at least one hard block S made of 95 to 100 wt.-% of vinyl aromatic monomers and 0 to 5 wt.-% dienes, one or more copolymer blocks (B/S) A , each made of 65 to 95 wt.-% of vinyl aromatic monomers and 5 to 35 wt.-% dienes and having a glass transition temperature Tg A in the range of 40° to 90°C and one or more copolymer blocks (B/S) B , each made of 20 to 60 wt.-% of vinyl aromatic monomers and 40 to 80 wt.-% dienes and having a glass transition temperature Tg B in the range of –70° to 0°C, c) 0 to 45 wt.-% of A and B of various thermoplastic polymers C and d) 0 to 6 wt.-% of processing aids D, wherein the total of A through D is 100 wt.-%, and use thereof for the production of shrink-wrap films.