Abstract:
A mixture comprising a) 5 to 95 wt.-% of a copolymer A that contains one or more copolymer blocks (B/S) A , each made of 65 to 95 wt.-% of vinyl aromatic monomers and 5 to 35 wt.-% dienes and having a glass transition temperature Tg A in the range of 40° to 90°C, b) 5 to 95 wt.-% of a block copolymer B containing at least one hard block S made of 95 to 100 wt.-% of vinyl aromatic monomers and 0 to 5 wt.-% dienes, one or more copolymer blocks (B/S) A , each made of 65 to 95 wt.-% of vinyl aromatic monomers and 5 to 35 wt.-% dienes and having a glass transition temperature Tg A in the range of 40° to 90°C and one or more copolymer blocks (B/S) B , each made of 20 to 60 wt.-% of vinyl aromatic monomers and 40 to 80 wt.-% dienes and having a glass transition temperature Tg B in the range of –70° to 0°C, c) 0 to 45 wt.-% of A and B of various thermoplastic polymers C and d) 0 to 6 wt.-% of processing aids D, wherein the total of A through D is 100 wt.-%, and use thereof for the production of shrink-wrap films.
Abstract:
The present invention relates to a surface treatment composition and a method for treating the surface of a substrate using the same. More particularly, the present invention relates to a surface treatment composition comprising a liquid medium as a main component, which prevents a substrate surface from being contaminated with metal impurities from the surface treatment composition and stably provides an extremely clean substrate surface, and also relates to a method fro treating the surface of a substrate by using the same. The composition comprises water, hydrogen peroxide, an alkaline compo und and 2 , 2-Bis- (hydroxyethyl) - (iminotris) - (hydroxymethyl) methan and/ or nitrilotriacetic acid.
Abstract:
The invention relates to a mixture, comprising a) 5 to 50 wt. % of a block copolymer (A), with one or more block copolymers (B/S)A, each made from 65 to 95 wt. % vinylaromatic monomers and 35 to 5 wt. % dienes with a glass transition temperature TgA in the range 40° to 90 °C, b) 95 to 50 wt. % of a block copolymer B, with at least one hard block (S) made from vinylaromatic monomers and one or more copolymer blocks (B/S)B, each made from 20 to 60 wt. % vinylaromatic monomers and 80 to 40 wt. % dienes and a glass temperature TgB in the range -70° to 0 °C, c) 0 to 45 wt. % of a block copolymer (C) different from (A) and (B), or polystyrol and d) 0 to 6 wt. % of a plastifier and the use thereof for the production of shrink films.