公开(公告)号:EP4021621A1
公开(公告)日:2022-07-06
申请号:EP20760881.1
申请日:2020-08-28
Applicant: BASF SE
Inventor: PRISSOK, Frank , AHLERS, Jürgen , DOROODIAN, Amir , HARMS, Michael
-
公开(公告)号:EP3781618A1
公开(公告)日:2021-02-24
申请号:EP19717941.9
申请日:2019-04-18
Applicant: BASF SE
Inventor: POESELT, Elmar , GUTMANN, Peter , RAPP, Florian Tobias , PRISSOK, Frank
-
公开(公告)号:EP3781615A1
公开(公告)日:2021-02-24
申请号:EP19717940.1
申请日:2019-04-18
Applicant: BASF SE
Inventor: POESELT, Elmar , GUTMANN, Peter , RAPP, Florian Tobias , PRISSOK, Frank
-
公开(公告)号:EP3700969A1
公开(公告)日:2020-09-02
申请号:EP18789179.1
申请日:2018-10-25
Applicant: BASF SE
Inventor: PRISSOK, Frank , HARMS, Michael
-
公开(公告)号:EP3694908A1
公开(公告)日:2020-08-19
申请号:EP18780144.4
申请日:2018-10-08
Applicant: BASF SE
Inventor: AHLERS, Juergen , PRISSOK, Frank , GRONWALD, Oliver , WEBER, Martin
-
公开(公告)号:EP3268421B1
公开(公告)日:2020-08-12
申请号:EP16707778.3
申请日:2016-03-03
Applicant: BASF SE
Inventor: PRISSOK, Frank , HARMS, Michael , SCHUETTE, Markus
-
-
公开(公告)号:EP3535316A1
公开(公告)日:2019-09-11
申请号:EP17787204.1
申请日:2017-10-25
Applicant: BASF SE
Inventor: PRISSOK, Frank , KARAPETYAN, Gnuni , KEMPFERT, Dirk
-
9.
公开(公告)号:EP3475352A1
公开(公告)日:2019-05-01
申请号:EP17731582.7
申请日:2017-06-21
Applicant: BASF SE
Inventor: KEPPELER, Uwe , BARTL, Juergen , AHLERS, Juergen , DAESCHLEIN, Christian , GUTMANN, Peter , PRISSOK, Frank
-
公开(公告)号:EP3122534A1
公开(公告)日:2017-02-01
申请号:EP15709176.0
申请日:2015-03-11
Applicant: BASF SE
Inventor: BOKERN, Stefan , PRISSOK, Frank , HARTWIG, Sebastian , PÖSELT, Elmar , GOESCHEL, Julia
CPC classification number: B29C61/003 , B29C61/06 , B29K2075/00 , C08G18/244 , C08G18/3206 , C08G18/3215 , C08G18/4244 , C08G18/4825 , C08G18/4854 , C08G18/4879 , C08G18/6674 , C08G18/6681 , C08G18/758 , C08G18/7671 , C08G2280/00
Abstract: The invention relates to a method for producing a molded body (FK), comprising producing a thermoplastic polyurethane, producing a molded body (FK*) from the thermoplastic polyurethane, heating the molded body (FK*) to a temperature below the temperature at which there is permanent deformability of the molded body (FK*) and above the switching temperature of the thermoplastic polyurethane, elongating the heated molded body (FK*) and thus obtaining a molded body (FK), and cooling the molded body (FK) to a temperature below the switching temperature of the thermoplastic polyurethane. The invention further relates to molded bodies that are or can be obtained in accordance with such a method. The thermoplastic polyurethane comprises a polyisocyanate composition, a chain extender, and a polyol composition having at least one bisphenol derivative selected from the group comprising bisphenol A derivatives having a molecular weight Mw of > 315 g/mol and bisphenol S derivatives having a molecular weight Mw of > 315 g/mol, wherein at least one of the OH groups of the bisphenol derivative is alkoxylated. The invention further relates to the use of a thermoplastic polyurethane to produce a molded body having a shape memory effect in a temperature from 20 °C to 120 °C.
Abstract translation: 本发明涉及一种生产成型体(FK)的方法,包括制备热塑性聚氨酯,从热塑性聚氨酯制造成型体(FK *),将成型体(FK *)加热至低于 成型体(FK *)具有永久变形性,并且高于热塑性聚氨酯的开关温度,延长加热成型体(FK *),从而获得成型体(FK),并将成型体(FK)冷却至 温度低于热塑性聚氨酯的开关温度。 本发明还涉及根据这种方法得到或可以获得的成型体。 热塑性聚氨酯包括多异氰酸酯组合物,扩链剂和具有至少一种双酚衍生物的多元醇组合物,所述双酚衍生物选自分子量Mw> 315g / mol的双酚A衍生物和分子量Mw > 315g / mol,其中双酚衍生物的至少一个OH基团被烷氧基化。 本发明还涉及使用热塑性聚氨酯来制造在20℃至120℃的温度下具有形状记忆效应的成型体。
-
-
-
-
-
-
-
-
-