摘要:
A polyethylene composition (PC) comprising a multimodal C2C4C6 terpolymer (PE) with a density of 910 to 930 kg/m 3 , wherein the polyethylene composition (PC) has: a) an MFR 2 of 0.5 to 3.0 g/10 min; b) eta 300 of 800 to 2,000 Pa.s; and c) (Mw/Mn) of 2.0 to 10.0.
摘要:
The invention relates to a foamable polymer composition comprising a polyolefin polymer which polyolefin polymer does not bear silane moieties and comprises 20 to 99.99 wt.% linear low density polyethylene, and a blowing agent in an amount of 0.01 to 3 wt.% based on the total foamable polymer composition, wherein the blowing agent consists of citric acid and/or derivatives of citric acid or mixtures thereof. Further the invention relates to a foamable polymer composition comprising a polyolefin polymer, and a blowing agent in an amount of 0.01 to 3 wt.% based on the total foamable polymer composition, wherein the blowing agent consists of expandable polymeric microspheres, and the composition does not comprise fluororesin. Further the invention relates to a foamed polymer composition obtained by foaming this foamable polymer composition. Further the invention relates to the use of the foamable composition or the foamed polymer composition for a layer of a cable and a cable comprising at least one layer which comprises the foamable polymer composition or the foamed polymer composition.
摘要:
The present invention relates to a process for manufacturing polyethylene-silane copolymer conducted in a plant comprising at least one compressor unit (10) and at least one reactor (30) being downstream of the compressor unit (10) the process comprising the steps of a) Feeding a first feed stream (1) comprising ethylene into the at least one compressor unit (10) and subsequently to the at least one reactor (30), and b1) Feeding a second feed stream (2) comprising at least one silane comonomer to the at least one reactor (30) as front feed and/or b2) Feeding a second feed stream (2) comprising at least one silane comonomer to the at least one reactor (30) at at least one location along the reactor (30).
摘要:
The present invention relates to a low density polyethylene having a molecular weight distribution Mw/Mn which is greater than 15, a storage modulus G' (5kPa) which is above 3000 and a vinylidene content which is at least 15 / 100k C, compositions, a process for production of the low density polyethylene, a continuous ethylene polymerization method for introducing vinylidene in a low density polyethylene, a method for an extrusion coating process, an article, e.g. an extrusion article, and use in extrusion coating.
摘要:
The present invention relates to a polyolefin composition with good resistance to degradation caused by chlorine dioxide-containing water and at the same time showing low migration of the used additives and its decomposition products, especially phenols, out of the composition. The present invention is also directed to a pipe made of such a polyolefin composition. The present invention further relates to the use of the polyolefin composition for the production of a pipe and to the use of a combination of particular types of antioxidants for increasing the resistance of a polyolefin composition against degradation caused by contact with chlorine dioxide-containing water and for maintaining at the same time a low migration of the used additives and its decomposition products, especially phenols, out of the polyolefin composition.
摘要:
The present invention concerns the use of carbon black for reducing the shrinkage of a polyolefin composition to below 0.9%, wherein the polyolefin composition comprises a polyolefin polymer, and carbon black in an amount of from 0.05 to 2 wt.% based on the total weight of the polyolefin composition.