摘要:
This invention relates to polyolefin compositions. In particular, the invention pertains to elastic polymer compositions that can be more easily processed on cast film lines, extrusion lamination or coating lines due to improved resistance to draw resonance. The compositions of the present invention preferably comprise an elastomeric polyolefin resin and a high pressure low density type resin.
摘要:
The invention is directed to a fiber comprising a low crystallinity polymer and a high crystallinity polymer, wherein the fiber is capable of undergoing plastic deformation upon elongation and wherein the low crystallinity polymer comprises at least one ethylene/±-olefin inter polymer.
摘要:
A fiber is obtainable from or comprises a blend of a propylene based polymer and an ethylene/α-olefin interpolymer characterized by an elastic recovery, Re, in percent at 300 percent strain and 1 cycle and a density, d, in grams/cubic centimeter, wherein the elastic recovery and the density satisfy the following relationship: Re >1481-1629(d). Such interpolymer can also be characterized by other properties. The fibers made therefrom have a relatively high elastic recovery and a relatively low coefficient of friction. The fibers can be cross-linked, if desired. Woven, knitted or non-woven fabrics can be made from such fibers.
摘要:
Described herein are composite compositions and methods for making such compositions. The composition includes or is the reaction product of a cellulosic material, an organic component, and a thermoplastic. Some useful organic components include a silane-containing polymer. Some of the compositions have improved physical properties such as tensile properties, improved strength, and reduced water absorption.
摘要:
A fiber is obtainable from or comprises an ethylene/α-olefm interpolymer characterized by an elastic recovery, Re, in percent at 300 percent strain and (1) cycle and a density, d, in grams/cubic centimeter, wherein the elastic recovery and the density satisfy the following relationship: Re >1481-1629(d). Such interpolymer can also be characterized by other properties. The fibers made therefrom have a relatively high elastic recovery and a relatively low coefficient of friction. The fibers can be cross-linked, if desired. Woven or non-woven fabrics can be made from such fibers.
摘要:
A fiber is obtainable from or comprises a propylene/α-olefin interpolymer characterized by an elastic recovery, Re, in percent at 300 percent strain and 1 cycle and a density, d, in grams/cubic centimeter, wherein the elastic recovery and the density satisfy the following relationship: Re >1481-1629(d). Such interpolymer can also be characterized by other properties. The fibers made therefrom have a relatively high elastic recovery and a relatively low coefficient of friction. The fibers can be cross-linked, if desired. Woven or non- woven fabrics can be made from such fibers.