The purpose of the present invention is to provide a crucible which has high viscosity at high temperature, and can be used for a long time, and can be manufactured at low cost, and a method of manufacturing the same. The composite crucible 10 is characterized in the use of mullite (3A1 2 O 3 •2SiO 2 ) as the basic material of the crucible. The composite crucible 10 has the crucible body 11 made of mullite material whose main component is alumina and silica, and a transparent vitreous silica layer 12 formed on the inner surface of the crucible body 11. The thickness of the transparent vitreous silica layer 12 is smaller than that of the crucible body 11. The crucible body 11 can be formed by the slip casting method, and the transparent vitreous silica layer 12 can be formed by the thermal spraying method.