Polyimide resin composition
    10.
    发明公开
    Polyimide resin composition 有权
    Polyimidharzzusammensetzung

    公开(公告)号:EP1013714A1

    公开(公告)日:2000-06-28

    申请号:EP98124559.0

    申请日:1998-12-22

    IPC分类号: C08L79/08

    CPC分类号: C08L79/08

    摘要: A polyimide resin composition is disclosed herein which comprises 5 to 60% by weight of a polyimide [polyimide (1)] having a repeating unit represented by the chemical formula 1 and 40 to 95% by weight of a polyimide [polyimide (2)] having a repeating unit represented by the chemical formula 2. According to the present invention, there are provided a polymer alloy in which the advantages of the polyimide (1) and the polyimide (2) are utilized and the disadvantages of the polyimide (1) and the polyimide (2) are reduced; a polyimide resin composition from which crystalline molded articles can be obtained even by a usual molding cycle, for example, an injection molding cycle of about 30 to 60 seconds; and a polyimide resin composition from which molded articles having an excellent dimensional accuracy and flexural modulus can be obtained even by a usual molding cycle, for example, an injection molding cycle of about 30 to 60 seconds, for example, in the case that the molded articles are intended to be used at a high temperature of 230°C or more, for example, a temperature of 230 to 300°C, or 230 to 250°C.

    摘要翻译: 本文公开了一种聚酰亚胺树脂组合物,其包含5至60重量%的具有由化学式1表示的重复单元的聚酰亚胺酰亚胺(1)和40至95重量%的聚酰亚胺Α聚酰亚胺(2) 根据本发明,提供了一种聚合物合金,其中使用聚酰亚胺(1)和聚酰亚胺(2)的优点,并且聚酰亚胺(1)和 聚酰亚胺(2)减少; 聚酰亚胺树脂组合物,甚至可以通过通常的模制循环,例如约30至60秒的注塑周期获得结晶模制品; 以及聚酰亚胺树脂组合物,即使在通常的成型周期(例如约30〜60秒的注射成型周期)下也可以得到具有优异的尺寸精度和挠曲模量的成型品,例如在成型 制品应在230℃以上的高温下使用,例如230〜300℃,230〜250℃的温度。