摘要:
A coil electric conductor (1) has an insulating substrate (2), a first conductive layer (3), and a second conductive layer (5). The first conductive layer (3) is formed at a depression (4) provided on a face of the insulating substrate (2). The second conductive layer (5) is formed on the first conductive layer (3) with the first conductive layer (3) interposed between the second conductive layer (5) and the insulating substrate (2). This construction realizes a coil electric conductor having a highly precisely uniformized cross-sectional shape.
摘要:
Soft magnetic powder of Fe-Al-Si system of which magnetostrictive constant λ takes a positive value at the room temperature is employed to produce a magnetic composite article so that a temperature characteristic of core-loss of the article takes a negative value at the room temperature. Excellent magnetic characteristics such as a low core-loss and a high permeability can be obtained at a high frequency band.
摘要:
Soft magnetic powder of Fe-Al-Si system of which magnetostrictive constant λ takes a positive value at the room temperature is employed to produce a magnetic composite article so that a temperature characteristic of core-loss of the article takes a negative value at the room temperature. Excellent magnetic characteristics such as a low core-loss and a high permeability can be obtained at a high frequency band.
摘要:
An oxide magnetic material provided by the present invention contains, as main components, 61 to 67 mol% of Fe₂O₃; 3 to 36 mol% of MnO; and 30 mol% or less of ZnO, and further contains, as sub-components, 0.05 to 0.5 wt% of CaO; and 0.005 to 0.2 wt% of SiO₂. Such materials can further contain one or more kinds of oxides selected from the group consisting of ZrO₂, HfO₂, Ta₂O₅, Cr₂O₃, MoO₃, WO₃, Al₂O₃, Ga₂O₃, In₂O₃, GeO₂, SnO₂, Sb₂O₃ and Bi₂O₃. Such magnetic materials of the present invention have the advantages of having an extremely low magnetic loss even when used in the high frequency band and having a minimum magnetic loss at a temperature sufficiently higher than room temperature. Moreover, a switching power supply having a switching frequency of 300 kHz to 5 MHz is provided by using such magnetic materials as a magnetic core.
摘要翻译:本发明提供的氧化物磁性材料以Fe 2 O 3为主要成分为61〜67摩尔%。 3〜36摩尔%的MnO; 和30摩尔%以下的ZnO,作为副成分,还含有0.05〜0.5重量%的CaO; 和0.005〜0.2重量%的SiO 2。 这些材料还可以含有选自ZrO 2,HfO 2,Ta 2 O 5,Cr 2 O 3,MoO 3,WO 3,Al 2 O 3,Ga 2 O 3,In 2 O 3,GeO 2,SnO 2,Sb 2 O 3和Bi 2 O 3中的一种以上的氧化物。 本发明的这种磁性材料具有即使在高频带下使用也具有非常低的磁损耗并且在足够高于室温的温度下具有最小的磁损耗的优点。 此外,通过使用这种磁性材料作为磁芯,提供具有300kHz至5MHz的开关频率的开关电源。
摘要:
The present invention provides a composite magnetic body containing metallic magnetic powder and thermosetting resin and having a packing ratio of the metallic magnetic powder of 65 vol% to 90 vol% and an electrical resistivity of at least 10 4 Ω•cm. When a coil is embedded in this composite magnetic body, a miniature magnetic element can be obtained that has a high inductance value and is excellent in DC bias characteristics.
摘要:
The present invention provides a composite magnetic body containing metallic magnetic powder and thermosetting resin and having a packing ratio of the metallic magnetic powder of 65 vol% to 90 vol% and an electrical resistivity of at least 10 4 Ω•cm. When a coil is embedded in this composite magnetic body, a miniature magnetic element can be obtained that has a high inductance value and is excellent in DC bias characteristics.
摘要:
An oxide magnetic material provided by the present invention contains, as main components, 55 to 59 mol% of Fe₂O₃; 35 to 42 mol% of MnO; and 6 mol% or less of ZnO, and further contains, as sub-components, 0.05 to 0.3 wt% of CaO; and 0.005 to 0.05 wt% of SiO₂. The other oxide magnetic material provided by the present invention contains, as main components, 61 to 67 mol% of Fe₂O₃; 3 to 36 mol% of MnO; and 30 mol% or less of ZnO, and further contains, as sub-components, 0.05 to 0.5 wt% of CaO; and 0.005 to 0.2 wt% of SiO₂. Such materials can further contain one or more kinds of oxides selected from the group consisting of ZrO₂, HfO₂, Ta₂O₅, Cr₂O₃, MoO₃, WO₃, Al₂O₃, Ga₂O₃, In₂O₃, GeO₂, SnO₂, Sb₂O₃ and Bi₂O₃. Such magnetic materials of the present invention have the advantages of having an extremely low magnetic loss even when used in the high frequency band and having a minimum magnetic loss at a temperature sufficiently higher than room temperature. Moreover, a switching power supply having a switching frequency of 300 kHz to 5 MHz is provided by using such magnetic materials as a magnetic core.
摘要翻译:本发明提供的氧化物磁性材料作为主要成分含有55〜59摩尔%的Fe 2 O 3, 35〜42mol%的MnO; 和6mol%以下的ZnO,作为副成分,进一步含有0.05〜0.3wt%的CaO; 和0.005〜0.05重量%的SiO 2。 本发明提供的另一种氧化物磁性材料以Fe2O3为主要成分为61〜67摩尔% 3〜36摩尔%的MnO; 和30摩尔%以下的ZnO,作为副成分,还含有0.05〜0.5重量%的CaO; 和0.005〜0.2重量%的SiO 2。 这些材料还可以含有选自ZrO 2,HfO 2,Ta 2 O 5,Cr 2 O 3,MoO 3,WO 3,Al 2 O 3,Ga 2 O 3,In 2 O 3,GeO 2,SnO 2,Sb 2 O 3和Bi 2 O 3中的一种以上的氧化物。 本发明的这种磁性材料具有即使在高频带下使用也具有非常低的磁损耗并且在足够高于室温的温度下具有最小的磁损耗的优点。 此外,通过使用这种磁性材料作为磁芯,提供具有300kHz至5MHz的开关频率的开关电源。
摘要:
An oxide magnetic material provided by the present invention contains, as main components, 55 to 59 mol% of Fe₂O₃; 35 to 42 mol% of MnO; and 6 mol% or less of ZnO, and further contains, as sub-components, 0.05 to 0.3 wt% of CaO; and 0.005 to 0.05 wt% of SiO₂. The other oxide magnetic material provided by the present invention contains, as main components, 61 to 67 mol% of Fe₂O₃; 3 to 36 mol% of MnO; and 30 mol% or less of ZnO, and further contains, as sub-components, 0.05 to 0.5 wt% of CaO; and 0.005 to 0.2 wt% of SiO₂. Such materials can further contain one or more kinds of oxides selected from the group consisting of ZrO₂, HfO₂, Ta₂O₅, Cr₂O₃, MoO₃, WO₃, Al₂O₃, Ga₂O₃, In₂O₃, GeO₂, SnO₂, Sb₂O₃ and Bi₂O₃. Such magnetic materials of the present invention have the advantages of having an extremely low magnetic loss even when used in the high frequency band and having a minimum magnetic loss at a temperature sufficiently higher than room temperature. Moreover, a switching power supply having a switching frequency of 300 kHz to 5 MHz is provided by using such magnetic materials as a magnetic core.
摘要翻译:本发明提供的氧化物磁性材料作为主要成分含有55〜59摩尔%的Fe 2 O 3, 35〜42mol%的MnO; 和6mol%以下的ZnO,作为副成分,进一步含有0.05〜0.3wt%的CaO; 和0.005〜0.05重量%的SiO 2。 本发明提供的另一种氧化物磁性材料以Fe2O3为主要成分为61〜67摩尔% 3〜36摩尔%的MnO; 和30摩尔%以下的ZnO,作为副成分,还含有0.05〜0.5重量%的CaO; 和0.005〜0.2重量%的SiO 2。 这些材料还可以含有选自ZrO 2,HfO 2,Ta 2 O 5,Cr 2 O 3,MoO 3,WO 3,Al 2 O 3,Ga 2 O 3,In 2 O 3,GeO 2,SnO 2,Sb 2 O 3和Bi 2 O 3中的一种以上的氧化物。 本发明的这种磁性材料具有即使在高频带下使用也具有非常低的磁损耗并且在足够高于室温的温度下具有最小的磁损耗的优点。 此外,通过使用这种磁性材料作为磁芯,提供具有300kHz至5MHz的开关频率的开关电源。