公开(公告)号:EP3196233A4
公开(公告)日:2018-06-20
申请号:EP15856571
申请日:2015-11-06
申请人: SUMITOMO RUBBER IND
发明人: YAMANA AYUKO , YOKOYAMA YUKA , NAKATANI MASAKO , MIKI TAKASHI , HORIGUCHI TAKUYA , MIZUNO YOICHI , KAWACHI TAKAHIRO , OKABE NOBORU , SUGIMOTO NATSUKI , UESAKA KENICHI , MAEKAWA TETSUYA , SUZUKI YUMI , KATO FUMIYA
IPC分类号: C08J3/20 , B29C35/02 , B60C1/00 , C07C279/02 , C08K3/36 , C08K5/103 , C08K5/372 , C08K5/54 , C08K5/548 , C08L7/00 , C08L9/00 , C08L9/06 , C08L21/00
CPC分类号: B60C1/0016 , B29C35/02 , B60C1/00 , C07C279/02 , C08J3/20 , C08K3/36 , C08K5/103 , C08K5/372 , C08K5/54 , C08K5/548 , C08K2201/006 , C08L7/00 , C08L9/00 , C08L9/06 , C08L21/00 , C08L2205/03
摘要: According to a production method of a rubber composition for tire of the present invention comprising a rubber component (A) comprising at least one selected from the group consisting of a natural rubber and a synthetic diene rubber, a filler, a coupling agent (D) represented by the following chemical formula (1), and a vulcanizing agent (E) comprising a vulcanizer and a vulcanization accelerator, the method comprising: (step X1) a step X1 of kneading all amount of A, a part of the filler and a part of D, (step X2) a step X2 of kneading the kneaded product of step X1, the remaining amount of the filler and D, and (step F) a step F of kneading the kneaded product of step X2 and E, it is possible to produce a rubber composition for tire in which fuel efficiency and abrasion resistance are improved in a good balance. Chemical formula (1): (C p H 2p+1 O) 3 -Si-(CH 2 ) q -S-CO-C k H 2k+1 In the chemical formula (1), p represents an integer of 1 to 3, q represents an integer of 1 to 5, and k represents an integer of 5 to 12.