NATURAL RUBBER-CONTAINING THERMOPLASTIC RESIN COMPOSITION AND MOLDED ARTICLE THEREOF
    1.
    发明公开
    NATURAL RUBBER-CONTAINING THERMOPLASTIC RESIN COMPOSITION AND MOLDED ARTICLE THEREOF 有权
    热塑性麻醉药HARZZUSAMMENSETZUNG MITNATÜRLICHEMKAUTSCHUK UNDFORMKÖRPERDARAUS

    公开(公告)号:EP2902440A4

    公开(公告)日:2016-05-04

    申请号:EP13841001

    申请日:2013-09-20

    Abstract: The present invention addresses the problem of providing a natural rubber-containing thermoplastic resin composition which uses a natural rubber latex and has physical properties achieving excellent balance among impact resistance, fluidity and color tone, without requiring a complicated deproteinization process for natural rubbers. A solution of the problem is a natural rubber-containing thermoplastic resin composition which contains a graft copolymer (A) that is obtained by graft polymerizing a vinyl monomer mixture (a), which contains at least an aromatic vinyl monomer, to a rubber polymer (R) that is formed of 10-70% by mass of a natural rubber having a weight average particle diameter within the range of 0.3-1.2 [mu]m and 30-90% by mass of a synthetic rubber having a weight average particle diameter within the range of 0.2-0.4 [mu]m. This natural rubber-containing thermoplastic resin composition is characterized in that: the natural rubber particles contain natural rubber particles having particle diameters of 1.0 [mu]m or more in an amount of 5% by mass or more; and the inner graft rate of the rubber polymer (R) particles having particle diameters of 1.0 [mu]m or more is 20% or more.

    Abstract translation: 本发明解决了提供使用天然橡胶胶乳的天然橡胶的热塑性树脂组合物的问题,并且具有在抗冲击性,流动性和色调之间达到优异平衡的物理性能,而不需要对天然橡胶进行复杂的脱蛋白处理。 该问题的解决方案是含天然橡胶的热塑性树脂组合物,其含有通过将含有至少一种芳族乙烯基单体的乙烯基单体混合物(a)接枝聚合到橡胶聚合物上而获得的接枝共聚物(A) R),其由10-70质量%的重均粒径在0.3-1.2μm范围内的天然橡胶和30-90质量%的具有重均粒径的合成橡胶 在0.2-0.4μm的范围内。 该含天然橡胶的热塑性树脂组合物的特征在于:天然橡胶粒子含有5质量%以上的粒径为1.0μm以上的天然橡胶粒子, 并且粒径为1.0μm以上的橡胶聚合物(R)颗粒的内接枝率为20%以上。

    THERMOPLASTIC RESIN COMPOSITION
    2.
    发明公开
    THERMOPLASTIC RESIN COMPOSITION 有权
    THERMOPLASTISCHE HARZZUSAMMENSETZUNG

    公开(公告)号:EP3103838A4

    公开(公告)日:2017-08-30

    申请号:EP15746984

    申请日:2015-01-29

    Abstract: A thermoplastic resin composition comprising a graft copolymer (I) which is produced by carrying out the graft polymerization of a monomer mixture (B) comprising an aromatic vinyl monomer and a vinyl cyanide monomer in the presence of an acrylic rubbery polymer (A) and a vinyl copolymer (II) which is produced by carrying out the copolymerization of an aromatic vinyl monomer with a vinyl cyanide monomer, wherein the ratio of the content of the former copolymer to that of the latter copolymer is (30 to 70 parts by weight) : (70 to 30 parts by weight), the graft copolymer (I) has such a property that the ratio (i.e., (±)/(²)) of the gel swelling degree (±) of the acrylic rubbery polymer (A) in toluene to the grafting ratio (²) of the graft copolymer (I) is 0.4 to 2.0, and the thermoplastic resin composition has such a structure that particles of the graft copolymer (I) are aggregated in the thermoplastic resin composition. From the thermoplastic resin composition, a molded article having excellent fluidability, weather resistance and impact resistance can be produced.

    Abstract translation: 一种热塑性树脂组合物,其特征在于,含有在丙烯酸类橡胶状聚合物(A)和丙烯酸类橡胶状聚合物(A)的存在下进行含有芳香族乙烯基单体和氰化乙烯基单体的单体混合物(B)的接枝聚合而得到的接枝共聚物 乙烯基共聚物(II),其是通过将芳香族乙烯基单体与氰化乙烯基单体进行共聚而得到的,其中前者的共聚物与后者的共聚物的含量之比为(30〜70重量份): (70〜30重量份)时,接枝共聚物(I)具有丙烯酸类橡胶状聚合物(A)的凝胶溶胀度(±)的比例(即(±)/(2) 甲苯与接枝共聚物(I)的接枝率(²)之比为0.4-2.0,并且热塑性树脂组合物具有这样的结构,即接枝共聚物(I)的颗粒聚集在热塑性树脂组合物中。 从热塑性树脂组合物可以制造具有优异的流动性,耐候性和耐冲击性的成型制品。