POLYMER FILM WITH RENEWABLE CONTENT
    5.
    发明公开
    POLYMER FILM WITH RENEWABLE CONTENT 审中-公开
    可更新内容的聚合物薄膜

    公开(公告)号:EP3003712A1

    公开(公告)日:2016-04-13

    申请号:EP14804932.3

    申请日:2014-05-29

    申请人: Tristano Pty Ltd

    发明人: LEUFGENS, Markus

    摘要: The present invention relates to polymer film having a multilayer structure, the multilayer structure comprising an inner polymer layer interposed between first and second outermost polymer layers, wherein: (i) the inner polymer layer comprises a melt blend of: (a) a starch containing polymer composition comprising polyethylene, thermoplastic starch, and one or more compatibilisers; (b) a metallocene polyethylene having a melt flow index in the range of 0.5 to 2.5 g/10min and a density in the range of 0.910 to 0.935 g/cm
    3 ; (c) polyethylene having a melt flow index in the range of 2 to 4 g/10min and a density in the range of 0.918 to 0.925 g/cm
    3 ; and (d) polyethylene have a melt flow index in the range of 0.05 to 0.2 g/10min and a density in the range of 0.948 to 0.955 g/cm
    3 ; (ii) the first and second outermost layers independently (a) comprise a metallocene polyethylene having a melt flow index in the range of 0.5 to 2.5 g/10min and a density in the range of 0.916 to 0.935 g/cm
    3 , or (b) have a heat seal initiation temperature of no greater than 120°C, wherein at least one of the first and second outermost layers has a heat seal initiation temperature of no greater than 120°C.

    摘要翻译: 本发明涉及具有多层结构的聚合物膜,所述多层结构包含插入第一和第二最外聚合物层之间的内聚合物层,其中:(i)内聚合物层包含以下物质的熔融共混物:(a)含淀粉 包含聚乙烯,热塑性淀粉和一种或多种相容剂的聚合物组合物; (b)熔体流动指数为0.5-2.5克/ 10分钟,密度为0.910-0.935克/厘米3的茂金属聚乙烯; (c)熔体流动指数在2至4g / 10min范围内且密度在0.918至0.925g / cm 3范围内的聚乙烯; 和(d)聚乙烯具有0.05-0.2g / 10min范围内的熔体流动指数和0.948-0.9555g / cm 3范围内的密度; (ii)第一和第二最外层独立地(a)包含熔体流动指数在0.5-2.5g / 10min范围内且密度在0.916-0.935g / cm 3范围内的茂金属聚乙烯,或(b) )具有不高于120℃的热封起始温度,其中第一和第二最外层中的至少一个具有不高于120℃的热封起始温度。