Bituminous compositions
    9.
    发明公开
    Bituminous compositions 有权
    Bitumenhaltige Zusammensetzungen

    公开(公告)号:EP2093274A1

    公开(公告)日:2009-08-26

    申请号:EP08101807.9

    申请日:2008-02-20

    申请人: CECA S.A.

    IPC分类号: C10C3/02 C08L95/00 C08K5/16

    摘要: This invention relates to the modification of bitumen by polymeric materials used particularly for the preparation of asphalt mixtures with enhanced mechanical properties, wherein the polymeric materials are selected from additives capable of forming a supramolecular assembly. The modified bitumen may be used for the fabrication of asphalts mixtures with mineral aggregates used in construction or maintenance of sidewalks, roads, highways, parking lots or airport runaways and service roads and any other rolling surfaces.

    摘要翻译: 本发明涉及通过特别用于制备具有增强的机械性能的沥青混合物的聚合材料改性沥青,其中聚合材料选自能够形成超分子组装的添加剂。 改性沥青可用于制造用于建筑或维护人行道,道路,高速公路,停车场或机场逃离道路以及服务道路和任何其他滚动表面的矿物聚集体的沥青混合物。

    ADSORBANTS ZEOLITIQUES AGGLOMERES, LEUR PROCEDE DE PREPARATION ET LEURS UTILISATIONS
    10.
    发明公开
    ADSORBANTS ZEOLITIQUES AGGLOMERES, LEUR PROCEDE DE PREPARATION ET LEURS UTILISATIONS 审中-公开
    AGGOMERIERTE ZEOLITISCHE ADSORPTIONSMITTEL,VERFAHREN ZU IHRER HERSTELLUNG UND IHRE VERWENDUNGEN

    公开(公告)号:EP2043775A1

    公开(公告)日:2009-04-08

    申请号:EP07823582.7

    申请日:2007-07-13

    IPC分类号: B01J20/18

    CPC分类号: B01J20/183 B01J20/186

    摘要: The present invention relates to agglomerated zeolitic adsorbents based on zeolite X with an Si/Al ratio such that 1.15

    摘要翻译: 包含钡X沸石粉末和惰性粘合剂的聚集的沸石吸附剂具有至少0.245cm 3> / g的Dubinin体积和至少2MPa的机械强度(Shell SMS1471-74)。 沸石粉末的晶体直径为1.6μm以下,硅/铝比为1.15-1.5,其中至少90%的阳离子交换位置被钡离子或钡和钾离子占据,条件是不再有 超过1/3的这些位点被钾离子所占据。 还包括以下独立权利要求:(1)通过将X沸石粉末与包含至少80重量%的可分解沸石的粘土和二氧化硅源的粘合剂凝聚在一起来生产吸附剂的方法(P1),干燥并煅烧附聚物, 用碱溶液粘合剂,用钡代替至少90​​%的交换位置,洗涤和干燥产物,任选地用钾取代最多33%的交换位点,并洗涤,干燥和活化产物,其中钾交换可以 在钡交换之前或之后进行; (2)通过如上所述在解吸剂的存在下通过在吸附剂上吸附来从液相或气相中的C 8芳族馏分中回收对二甲苯的方法(P2)。