摘要:
The invention relates to a method for the desalination of a polymer (sP) containing salt, said polymer containing a polyaryl ether and a salt (S). Said method comprises the following steps a) the surface of the salt-containing polymer (sP) is mechanically enlarged to obtain a surface-enlarged salt-containing polymer (osP), b) the surface-enlarged, salt-containing polymer (osP) from step (a) is brought into contact with an extraction agent (E) to obtain a desalinated polymer (eP) which contains the polyaryl ether, and a salt-containing extraction agent (sE) which contains the extraction agent (E) and the salt (S).
摘要:
[Problem to be Solved] An object of the present invention is to provide a polyphenylene ether powder that has a high loose apparent specific gravity and good handleability, as well as a high solvent solubility, and good covering properties by coating, applying and the like, and further, when formed as a covering film, providing the covering film with excellent mechanical properties. [Solution] The polyphenylene ether powder according to the present invention has a loose apparent specific gravity of 0.40 or more and 0.85 or less, and includes 5 to 20 mass% of a component having a molecular weight of 50,000 or more and 12 to 30 mass% of a component having a molecular weight of 8,000 or less.
摘要:
The present invention is directed to a process for preparing halogen-free melt-filtered polymer compositions, compositions prepared by the process, as well as articles derived therefrom. The process comprises filtering the melted composition through a filter to remove particulate impurities that are 0.5 mm2 in size or larger. The composition comprises: (a) 60 to 90 percent by weight of a poly(phenylene ether); (b) 3 to 23 percent by weight of a styrenic polymer; (c) 5-11 percent by weight of a halogen-free flame retardant comprising at least one organic phosphate flame retardant, wherein the composition has: (i) a melt viscosity of 620 Pa·s or less as measured according at 280° C. and 1500 s−1; and (ii) a heat deflection temperature that is 135° C. or more as measured according to ASTM D648 on 6.4 mm thick bars at 1.82 MPa.
摘要:
The invention relates to a method for processing polymer solutions comprising N-methyl-2-pyrrolidone and a polymer, the polymer solution being hydrogenated in the presence of a hydrogenation catalyst using hydrogen. The invention also relates to the product that can be obtained by this method and to the use of said product for producing, in particular, polyarylene ether products.
摘要:
The present invention provides a cyclic poly (phenylene ether ether ketone) composition comprising not less than 60% by weight of a cyclic poly (phenylene ether ether ketone) represented by the following Formula (I), which is characterized in that the cyclic poly (phenylene ether ether ketone) is a mixture of cyclic poly (phenylene ether ether ketone)s having different repeating numbers (m) and the composition has a melting point of not higher than 270°C; and a method of producing a poly (phenylene ether ether ketone) characterized by heat-polymerizing the cyclic poly (phenylene ether ether ketone) composition: