ONE-PACK TYPE UNHARDENING ADHESIVE FILM WATERPROOFING MATERIAL USING WASTE RUBBER AND METHOD FOR MANUFACTURING SAME
    5.
    发明公开
    ONE-PACK TYPE UNHARDENING ADHESIVE FILM WATERPROOFING MATERIAL USING WASTE RUBBER AND METHOD FOR MANUFACTURING SAME 审中-公开
    接合膜从ONE PIECE软化剂和生产具有废橡胶和处理防水材料

    公开(公告)号:EP2562224A1

    公开(公告)日:2013-02-27

    申请号:EP11838125.0

    申请日:2011-02-16

    摘要: Disclosed therein is a non-curing one-component adhesive waterproof material using scrap rubber and a preparation method thereof in which scrap rubber is mixed with oil, heated and pulverized into size-reduced rubber under mechanical shear stress, and more particularly, to a non-curing one-component adhesive waterproof material using scrap rubber and a preparation method thereof in which scrap rubber is heated to have a reduced elasticity, pulverized into size-reduced rubber under mechanical shear stress, and then mixed with emulsified asphalt, styrene butadiene rubber (SBR), and natural rubber (NR).
    The present invention includes: 10 to 15 parts by weight of scrap rubber chips; 20 to 25 parts by weight of oil, the scrap rubber chips and the oil being mixed together, heated at 200 to 230 °C and then subjected to size reduction under mechanical shear stress to pulverize the scrap rubber chips into size-reduced rubber; and 29.6 to 40 parts by weight of emulsified asphalt being mixed with the size-reduced rubber. The mixture of the emulsified asphalt and the size-reduced rubber is mixed with 8 to 13 parts by weight of a filler, 1 to 2 parts by weight of a surfactant, and 0.1 to 0.4 part by weight of an anti-ageing agent at a temperature of 90 to 100 °C, and then further mixed with 3 to 6 parts by weight of SBR and 5 to 9 parts by weight of NR for viscosity control.

    摘要翻译: 其中公开的是一个非固化使用废胶和其制备方法,其中废胶与油混合,加热和粉碎成机械剪切应力下减小尺寸橡胶,并且更具体的单组分粘合剂防水材料,对非 使用废胶和其制备方法在其中废胶被加热以具有减小的弹性,粉碎成机械剪切应力下减小尺寸橡胶,然后用乳化沥青混合,苯乙烯 - 丁二烯橡胶-curing单组分粘合剂的防水材料( SBR)和天然橡胶(NR)。 本发明包括:10至15重量份的废胶芯片; 20至25重量份的油,废胶芯片和油混合在一起,加热到200至230℃,然后进行机械剪切应力以粉碎废胶芯片到尺寸减小的橡胶下减小尺寸; 和6.29至40重量份的乳化沥青与所述尺寸减小的橡胶混合。 乳化沥青和尺寸减小的橡胶的混合物用8至13重量份的填料的重量抗老化剂中的一个混合,1〜2重量份的表面活性剂,和0.1至0.4份 的温度90〜100℃,然后用3继6重量份的SBR和5到9重量份的NR用于粘度控制混合。