SURFACE TREATMENT AGENT
    7.
    发明公开

    公开(公告)号:EP4501471A1

    公开(公告)日:2025-02-05

    申请号:EP23779636.2

    申请日:2023-03-15

    Abstract: A surface treatment agent capable of forming a film that has excellent corrosion resistance and hydrophilicity with suppressed odor is provided. A surface treatment agent includes: one or more selected from water-soluble inorganic oxides and salts thereof (A); one or more selected from hydrolysates and condensates of organoalkoxysilane (B); water-soluble resin (C); ether compound (D); and water and/or water-miscible solvent; wherein assuming a total mass of the one or more selected from water-soluble inorganic oxides and salts thereof (A), a total mass of the one or more selected from hydrolysates and condensates of organoalkoxysilane (B), a mass of the water-soluble resin (C), and a mass of the ether compound (D) are M A , M B , M C and M D , respectively, (M A + M B ) / (M A + M B + M C + M D ) = 0.01 to 0.7 is satisfied.

    METHOD FOR FORMING MULTILAYER COATING FILM
    9.
    发明公开

    公开(公告)号:EP4474063A1

    公开(公告)日:2024-12-11

    申请号:EP23749579.1

    申请日:2023-01-23

    Abstract: The purpose of the present invention is to provide a method for forming a multilayer coating film which makes it possible to form a multilayer coating film having excellent metallic mottling resistance. The method for forming a multilayer coating film comprises: (1) a step for applying a first aqueous coating material (P1) on an object to be coated to form a first coating film; (2) a step for applying a second aqueous colored coating material (P2) on the first coating film to form a second colored coating film that contains a binder component (Ap2) and a lustrous pigment (Bp2); (3) a step for applying a clear-coat coating material (P3) on the second colored coating film to form a clear-coat coating film; and (4) a step for heating a multilayer coating film that includes the first coating film, the second colored coating film, and the clear-coat coating film so as to cure the multilayer coating film all at once. The first aqueous coating material (P1) contains a compound (A) that has a hydroxyl group and an acid group and that has an acid value of 50-150 mgKOH/g, a hydroxyl value of 100-300 mgKOH/g, and a weight-average molecular weight of 500-8,000, a film-forming resin (B), and a crosslinking agent (C).

Patent Agency Ranking