摘要:
A method of manufacturing stab-resistant fabric using water punching is provided. Aramid fabric and nonwoven aramid fabric are combined through water punching, thereby enhancing activities by ensuring flexibility and stab-resistance performance, and the method is an aramid composite fabric manufacturing method which performs water punching with pressure of 50 to 250 bar when the water punching is performed.
摘要:
Provided is a heat-resistant resin composite excellent in heat resistance and bending properties. This heat-resistant resin composite is constituted of a matrix resin and reinforcing fibers dispersed in the matrix resin. The matrix resin is constituted of a heat-resistant thermoplastic polymer having a glass transition temperature of 100°C or higher, and a polyester-based polymer comprising a terephthalic acid unit (A) and an isophthalic acid unit (B) at a copolymerization proportion (molar ratio) of (A)/(B) = 100/0 to 40/60. The proportion of the heat-resistant thermoplastic polymer in the composite is 30 to 80 wt%.
摘要:
The invention provides a process comprising heating a polyamic acid fiber to a temperature in the range of a first temperature and a second temperature for a period of time in the range of 5 seconds to 5 minutes to form a polyimide fiber, wherein the first temperature is the imidization temperature of the polyamic acid and the second temperature is the decomposition temperature of the polyimide
摘要:
A hot press cushioning material (14a) includes: a first nonwoven fabric (15) forming an inner layer; and second nonwoven fabrics (16a, 16b) placed on both surfaces of the first nonwoven fabric (15) and forming outer layers. Copolymerized para-aramid fibers having a basis weight of 80 to 400 g/m 2 are used as a material of the second nonwoven fabrics (16a, 16b). Fibers that are more rigid than the copolymerized para-aramid fibers are used as a material of the first nonwoven fabric (15). Each of the first nonwoven fabric (15) and the second nonwoven fabrics (16a, 16b) has a heat resistant temperature of 270°C or more.
摘要:
A consolidated fibrous mat comprises 20 to 50 weight percent of reinforcing fibers; and a continuous phase connecting the reinforcing fibers, comprising 50 to 70 weight percent of a polymer having a melt temperature at least 20°C lower than the reinforcing fibers, and 5 to 10 weight percent of a binder having a melt temperature lower than the polymer; wherein the weight percent of each of the reinforcing fibers, the polymer, and the binder is based on the combined total weight of the reinforcing fibers, the polymer, and the binder.