公开(公告)号:JP5011668B2
公开(公告)日:2012-08-29
申请号:JP2005212536
申请日:2005-07-22
Applicant: 東洋紡績株式会社
Inventor: 健二 柏原
CPC classification number: C08J3/05 , C08F8/14 , C08F8/32 , C08F8/46 , C08F255/02 , C08F255/04 , C08F2800/10 , C08J2351/06 , C08K3/30 , C08K5/06 , C08K5/17 , C08L51/06 , C08L2666/02 , C09D151/06 , C09J151/06 , C08F210/16 , C08F222/06
Abstract: A polyolefin wax-containing aqueous resin composition that can provide excellent properties without the use of a surfactant is provided. The aqueous resin composition is obtained by heating and dissolving 100 parts by mass of a carboxyl group-containing polyolefin wax in the presence of 15 to 67 parts by mass of a compound that satisfies general formula (1) shown below, and 90 to 380 parts by mass of water, and then dispersing this with a basic compound that has been added at a ratio of 1 to 4 chemical equivalents per carboxyl group of the carboxyl group-containing polyolefin wax. €ƒ€ƒ€ƒ€ƒ€ƒ€ƒ€ƒ€ƒGeneral Formula (1) C m H 2m+1 -(OCH 2 CH 2 ) n -OH m: an integer from 4 to 6, n: an integer from 1 to 4
-
公开(公告)号:JP5011669B2
公开(公告)日:2012-08-29
申请号:JP2005212537
申请日:2005-07-22
Applicant: 東洋紡績株式会社
CPC classification number: C08J3/05 , C08F8/22 , C08F8/44 , C08F2800/10 , C08J2351/06 , C08K5/06 , C08L51/06 , C08L71/02 , C08L2666/02 , C09D151/06 , C09J151/06 , C08L23/28 , C08L2666/14 , C08F255/02 , C08F255/04 , C08F222/06
Abstract: An aqueous resin composition that can provide excellent properties using a high molecular weight resin and less amount of surfactant, and also that does not require a complicated production procedure, is provided. The aqueous resin composition is obtained by heating and dissolving 100 parts by mass of acid-modified chlorinated polyolefin with an average molecular weight of 37,000 to 150,000 in the presence of 2 to 30 parts by weight of a surfactant, 10 to 50 parts by mass of a glycol ether-based compound that satisfies general formula (1) shown below, and 150 to 425 parts by mass of water, and then dispersing this with a basic compound that has been added at a ratio of 1 to 4 chemical equivalents per carboxyl group of the acid-modified chlorinated polyolefin. €ƒ€ƒ€ƒ€ƒ€ƒ€ƒ€ƒ€ƒGeneral Formula (1) C 4 H 9 -(OCH 2 CH 2 ) n -OH n: an integer from 1 to 4
-