摘要: 본발명은, 희토류원소불화물입자의외형의종횡비가 2 이하, 평균입자직경이 10㎛이상 100㎛이하, 벌크밀도가 0.8g/cm이상 1.5g/cm이하이며, 탄소를 0.1질량% 이상 0.5질량% 이하함유하는희토류원소불화물분말용사재료에관한것이다. 본발명에따르면, 대기중 플라즈마용사에적합한희토류원소불화물분말용사재료를얻을수 있다. 본발명의희토류원소불화물분말용사재료를사용하여제조한희토류원소불화물용사부재는할로겐가스중에서의내플라즈마부재로서사용했을경우, 부분적인색의변화가적고, 본래의긴 수명을실현할수 있는부재가된다.
-
公开(公告)号:KR1020160137519A
公开(公告)日:2016-11-30
申请号:KR1020167022994
申请日:2015-03-25
申请人: 가부시키가이샤 도쿠야마
IPC分类号: H01M8/1016 , H01M8/1004 , H01M8/083 , H01B1/06 , H01B1/04 , C01F17/00 , C01G3/00 , C01G3/02 , C01G9/00
CPC分类号: H01M8/1016 , C01F17/00 , C01F17/0043 , C01F17/005 , C01F17/0075 , C01G3/00 , C01G3/02 , C01G3/08 , C01G9/00 , C01G9/02 , C01P2002/22 , C01P2002/72 , C01P2004/61 , C01P2004/62 , C01P2004/64 , C01P2006/40 , C01P2006/60 , H01B1/04 , H01B1/06 , H01M2/1646 , H01M4/926 , H01M8/083 , H01M12/08 , H01M2300/0014 , H01M2300/0068 , Y02E60/128
摘要: [과제] 본발명은층상금속수산화물로이루어지는연료전지등의알칼리전해질막으로서사용할수 있는신규한음이온전도체를제공한다. [해결수단] 하기식(1)로표시되는층상금속수산화물의성형체로이루어지는것을특징으로하는음이온전도체. (M(OH)(A)-nHO) ... (1) (식중, M은 2가또는 3가의양이온이되는금속이고, α는금속 M의가수(價數)이고, A는음이온이되는원자또는원자단이며, z는음이온 A의가수이고, (αx-y)/z가 2 이상인경우, A는각각동일한가수의음이온이되는다른종류의음이온이어도되고, 다른가수의음이온이어도되며, n은 1 반복단위당포함되는층간수의평균분자수를의미한다.) 본발명의음이온전도체는무기물로구성되므로, 내열성, 물리적강도가우수하고, 연료전지또는공기전지용등의음이온전도체로서이용한때, 종래보다높은온도에서장시간작동시키는것이가능하다.
摘要翻译: 本发明提供一种新颖的阴离子导体,其包含层状金属氢氧化物,可用作燃料电池等中使用的碱性电解质膜。 [解决方案]阴离子导体,其特征在于包含由式(1)表示的层状金属氢氧化物的模制产物:[M x(OH)y(A)(αx-y)/ z-nH 2 O](其中M表示 可以用作二价或三价阳离子;α表示金属M的化合价数,A表示可用作阴离子的原子或原子团,z表示阴离子A的化合价数,其中,当 (αx-y)/ z为2以上时,A可以是可以作为彼此具有相同价值的阴离子的不同类型的阴离子,也可以是彼此不同价的阴离子,n表示 每个重复单元含有夹层水分子)。 根据本发明的阴离子导体由无机材料组成,因此具有优异的耐热性和物理强度,并且当用作燃料的阴离子导体时,可以在较高温度下与常规操作相比较长时间运行 电池,气泡等。
-
公开(公告)号:KR1020160038834A
公开(公告)日:2016-04-07
申请号:KR1020150137050
申请日:2015-09-25
申请人: 주식회사 엘지화학
摘要: 본명세서는 2종이상의금속산화물을반응시켜제조된복합금속산화물입자및 이의제조방법에관한것이다.
摘要翻译: 本发明涉及通过使两种以上的金属氧化物反应而制造的混合金属氧化物粒子及其制造方法。 混合金属氧化物颗粒包含由化学式1表示的第一混合金属氧化物La_(1-x)Q_xGa_(1-y)Z_yO_(3-δ); 和由化学式2 LaQGa_oO_p表示的第二混合金属氧化物。 混合金属氧化物颗粒的粒度分布均匀。
-
公开(公告)号:KR1020100122226A
公开(公告)日:2010-11-22
申请号:KR1020090041162
申请日:2009-05-12
申请人: 한화케미칼 주식회사
摘要: 본발명은졸-겔법을이용하여유기용매와디스프로슘-유기물복합체를반응시켜유기성분인계면활성제가산화디스프로슘(DyO, Dysprosium oxide) 나노입자의표면에코팅된나노판형상의산화디스프로슘의제조방법에관한것으로서, 본발명은공지된종래의기술보다낮은온도에서단순한공정으로균일한 DyO나노입자를제조할수 있기때문에생산비용을절감할수 있으며, 또한단분산된산화디스프로슘나노입자의모양이나노판(nano-plate)의형태를갖추고있음으로써다양한촉매제로의활용이가능하다.
摘要翻译: 目的:提供纳米板氧化镝纳米颗粒的制造方法,通过形成镝 - 有机复合物溶液和与有机溶剂进行溶胶 - 凝胶反应,提高纳米颗粒的纳米板形状的均匀性。 构成:纳米板氧化镝纳米颗粒的制造方法包括以下步骤:将镝前体和表面活性剂溶解在水和选自C 6〜C 30烃,C 1〜C 10醇的有机溶剂的混合溶液中, C5〜C30醚,形成镝 - 有机复合络合物; 将镝有机化合物络合物溶解在含有非共价电子对的有机溶剂中; 并加热获得纳米板氧化镝纳米颗粒。
-
公开(公告)号:KR1020100084318A
公开(公告)日:2010-07-26
申请号:KR1020090003746
申请日:2009-01-16
申请人: 삼성전자주식회사 , 삼성에스디아이 주식회사
CPC分类号: C01F17/00
摘要: PURPOSE: A ceria nano particle and a manufacturing method thereof are provided to manufacture a spherical ceria nano particle with the uniform size under 5 nanometers with a simple process. CONSTITUTION: A manufacturing method of a ceria nano particle comprises the following steps: obtaining a mixed solution by inserting a ceria precursor to a solution including monovalent alcohol with 1~5 carbons and water ; and irradiating gamma rays to the mixed solution. The mixture volume ratio of the alcohol and water is 0.01:1~0.2:1. The monovalent alcohol with 1~5 carbons is methanol, ethanol, butanol, isopropanol, or their mixture.
摘要翻译: 目的:提供二氧化铈纳米颗粒及其制造方法,以简单的方法制造具有均匀尺寸的球形二氧化铈纳米颗粒,其尺寸在5纳米以下。 构成:二氧化铈纳米颗粒的制造方法包括以下步骤:通过将二氧化铈前体插入到含有1〜5个碳原子的一价醇和水的溶液中来获得混合溶液; 并将γ射线照射到混合溶液中。 醇和水的混合体积比为0.01:1〜0.2:1。 具有1〜5个碳原子的一元醇是甲醇,乙醇,丁醇,异丙醇或它们的混合物。
-
公开(公告)号:KR1020100012824A
公开(公告)日:2010-02-08
申请号:KR1020090067574
申请日:2009-07-24
申请人: 주식회사 엘지화학
CPC分类号: C01F17/0043 , C01F17/005 , C01P2002/72 , C01P2004/03 , C01F17/00 , C01B32/60
摘要: PURPOSE: A fabricating method of a carium carbonate and a cerium oxide powder is provided to selectively manufacture the carium carbonate with a required crystal structure, kind and shape easily. CONSTITUTION: A manufacturing method of the carium carbonate comprises the steps of: mixing a cerium precursor and an urea; and reacting the cerium precursor and the urea by increasing the temperature to 50 ~ 250 degree Celsius the solvent-free condition. The cerium precursor and the urea are mixed in solid condition. The cerium precursor comprises a nitrate of the cerium, a sulphate, and a chloride or a ammonium salt. The reaction of the cerium precursor and the urea is processed under the pressure of 1~2 atm. The cerium precursor and the urea are mixed to the equivalence ratio of 1:0.5~1:10.
摘要翻译: 目的:提供碳酸铯和氧化铈粉末的制造方法,以选择性地制造所需的晶体结构,种类和形状的碳酸铯。 构成:碳酸铯的制造方法包括以下步骤:将铈前体和尿素混合; 并通过将温度升高到50〜250摄氏度的无溶剂条件使铈前体和尿素反应。 铈前体和尿素在固体条件下混合。 铈前体包括铈的硝酸盐,硫酸盐和氯化物或铵盐。 铈前体和尿素的反应在1〜2atm的压力下进行处理。 将铈前体和尿素混合至当量比为1:0.5〜1:10。
-
公开(公告)号:KR1019910010127B1
公开(公告)日:1991-12-17
申请号:KR1019870002809
申请日:1987-03-26
申请人: 로디아 쉬미
IPC分类号: C01F17/00
CPC分类号: C01F17/0012 , B01J23/10 , B01J35/1014 , B01J35/1019 , B01J35/1038 , B01J35/1061 , B01J35/1085 , C01F17/00 , C01F17/0043 , C01F17/0075 , C01P2006/13 , C01P2006/14 , C01P2006/16
摘要: 내용 없음.
-
公开(公告)号:KR1020160038832A
公开(公告)日:2016-04-07
申请号:KR1020150137046
申请日:2015-09-25
申请人: 주식회사 엘지화학
CPC分类号: H01M8/1246 , C01F5/00 , C01F11/00 , C01F17/00 , C01F17/0018 , C01G15/006 , C01P2002/34 , C01P2002/50 , C01P2002/72 , C01P2002/74 , C01P2004/51 , C01P2004/61 , C01P2006/40 , H01M2008/1293 , H01M2300/0074 , H01M2300/0091 , Y02E60/523 , Y02E60/525 , Y02P70/56
摘要: 본명세서는 2종이상의금속산화물을반응시켜제조된복합금속산화물입자및 이의제조방법에관한것이다.
摘要翻译: 本发明涉及通过使两种以上的金属氧化物反应而制造的混合金属氧化物粒子及其制造方法。 混合金属氧化物颗粒包含由化学式1表示的第一混合金属氧化物La_(1-x)Q_xGa_(1-y)Z_yO_(3-δ); 由化学式2 LaQGaO_4表示的第二混合金属氧化物; 和由化学式3 LaZGa_3O_7表示的第三混合金属氧化物。 混合金属氧化物颗粒的粒度分布均匀。
-
公开(公告)号:KR101522226B1
公开(公告)日:2015-05-26
申请号:KR1020140129424
申请日:2014-09-26
申请人: 한국과학기술연구원
CPC分类号: C09K11/08 , C01F17/00 , C01P2002/72 , C01P2004/03 , C01P2006/60 , C09K11/55 , C09K11/60 , C09K11/77 , C09K11/7728 , C09K11/7766 , C09K11/7783 , H01L31/055 , H01L33/502 , Y02E10/52
摘要: 본발명은비수용성금속수산화물의신규한제조방법및 이의용도에관한것이다. 본발명의비수용성금속수산화물은두 차례의고온열처리단계및 수세단계를통해간단하고효율적으로제조되어소량의알칼리금속을함유하며높은결정성과상 순도(phase purity)를가진다. 또한, 본발명의비수용성금속수산화물또는금속산화물은낮은파장대의흡수파장(예컨대, 490 nm 이하) 및높은파장대의발광파장(예컨대, 500 nm 이상 1100 nm 이하)을나타낸다. 따라서, 본발명의비수용성금속수산화물은다양한적용들, 예컨대소화제, 제산제, 흡착제등으로효율적으로이용될수 있을뿐 아니라, 다른금속이온으로도핑함으로써촉매, 형광체, 전극재료, 이차전지등의제조를위한원료소재로이용될수 있다.
摘要翻译: 本发明涉及非水金属氢氧化物的新颖制造方法及其用途。 本发明的非水金属氢氧化物通过高温热处理步骤和洗涤步骤简单有效地制造,从而含有少量碱金属并具有高结晶度和相纯度。 此外,本发明的非水金属氢氧化物或金属氧化物表示低波长带(例如490nm以下)的吸收波长和高波长带(例如500nm)的发光波长 至1100nm)。 因此,本发明的非水金属氢氧化物可以有效地用于各种应用中,例如消化药,抗酸剂,吸收剂等,并且可以用作制造催化剂的原料, 荧光物质,电极材料,二次电池等,通过掺杂不同的金属离子。
-
10.재활용 전해질 분말을 포함하는 고체산화물연료전지용 전해질 분말 및 이를 이용한 전해질 소결체 无效
标题翻译: 电解质粉末,包括用于固体氧化物燃料电池的再循环电解质粉末和由其制成的烧结电解质公开(公告)号:KR1020150030173A
公开(公告)日:2015-03-19
申请号:KR1020140119211
申请日:2014-09-05
申请人: 주식회사케이세라셀
CPC分类号: Y02P70/56 , H01M8/1253 , C01F17/00 , C01G25/00 , H01M8/02 , Y02E60/521 , Y02E60/525
摘要: 본 발명은 고 이온 전도성 전해질로서 최근 사용이 점차 확산되고 있지만 고가의 Sc 물질이 적용되는 ScSZ계 SOFC 전해질 소결체를 전해질 분말로 재활용하여 신규 합성한 YbScSZ 전해질 분말과 균일 복합체 전해질 분말로 제공하고 최종 SOFC용 전해질 소결체로 제조하는 것이며, 상기 복합 안정화 지르코니아 전해질 중의 산화물 질량 비율은 신규 합성 YbScSZ/재활용 ScSZ계가 1∼4인 것을 특징으로 하는 복합 안정화 지르코니아 전해질에 관한 것으로, 결과적으로 재활용된 ScSZ계 전해질 분말을 신규 합성한 YbScSZ 전해질 분말과 복합 분말로서 SOFC용 전해질로 구성함으로써 고 이온 전도성 전해질 소재의 가격 경쟁력을 높이고, 기존 YbScSZ 전해질의 산소이온 전도도를 유지 또는 향상시키는 장점과 ScSZ계 전해질의 환원 분위기 안정성이 개선되는 장점을 동시에 � �는 복합 안정화 지르코니아 전해질의 제공을 특징으로 한다.
摘要翻译: 本发明涉及作为电解质粉末作为高度离子传导性电解质的ScSZ系烧结SOFC电解质,作为新合成的YbScSZ电解质粉末的均匀复合电解质粉末而提供的复合稳定化氧化锆电解质, 广泛使用但具有施加高价格的Sc材料,并且用于制造用于SOFC的最终烧结电解质,其中根据新合成的YbScSZ,复合稳定氧化锆电解质中的氧化物的质量比为1〜4 到回收的ScSZ。 结果,本发明提供了一种复合稳定的氧化锆电解质,其提高了高离子传导性电解质材料的价格竞争力,并保持或提高了传统YbScSZ电解质的氧离子传导率,同时提高了ScSZ型电解质的还原气氛稳定性 通过配置回收的ScSZ基电解质粉末和新合成的YbScSZ电解质粉末作为SOFC的电解质的复合粉末。
-
-
-
-
-
-
-
-
-