Carbon Steel Sheet Superior in Formability and Manufacturing Method Thereof
    4.
    发明申请
    Carbon Steel Sheet Superior in Formability and Manufacturing Method Thereof 有权
    碳钢板的成型性和制造方法优越

    公开(公告)号:US20080295923A1

    公开(公告)日:2008-12-04

    申请号:US12158961

    申请日:2006-12-26

    IPC分类号: C21D8/00 C22C38/04

    摘要: A carbon steel sheet having high formability due to a microscopic and uniform carbide distribution and having a good characteristic of final heat treatment, and a manufacturing method thereof. The carbon steel sheet having excellent formability, includes, in wt %, C at 0.2-0.5%, Mn at 0.1-1.2%, Si at less than or equal to 0.4%, Cr at less than or equal to 0.5%, Al at 0.01-0.1%, S at less than or equal to 0.012%, Ti at less than or equal to 0.5×48/14×[N]% when the condition of B(atomic %)/N(atomic %)>1 is satisfied or by 0.5×48/14×[N]% to 0.03% when the condition of B and N is not satisfied, B at 0.0005-0.0080%, N at less than or equal to 0.006%, Fe, and extra inevitable elements; an average size of carbide is less than or equal to 1 μm; and an average grain size of ferrite is less than or equal to 5 μm.

    摘要翻译: 由于碳化物分布微观均匀而具有良好的最终热处理特性的高成形性碳钢板及其制造方法。 具有优异成形性的碳钢板以重量%计含有0.2-0.5%的C,0.1-1.2%的Mn,小于或等于0.4%的Si,小于或等于0.5%的Cr,小于或等于0.5%的Cr 0.01-0.1%,小于或等于0.012%的S,当满足B(原子%)/ N(原子%)> 1的条件时小于或等于0.5×48/14×[N]%的Ti或 当不满足B和N的条件时,为0.5×48/14×[N]%至0.03%,B为0.0005-0.0080%,N为小于或等于0.006%,Fe为额外不可避免的元素; 碳化物的平均尺寸小于或等于1um; 铁素体的平均粒径小于或等于5μm。

    HIGH CARBON STEEL SHEET SUPERIOR IN FATIUGUE LIFEAND MANUFACTURING METHOD THEREOF
    6.
    发明申请
    HIGH CARBON STEEL SHEET SUPERIOR IN FATIUGUE LIFEAND MANUFACTURING METHOD THEREOF 审中-公开
    高碳钢生产线的高碳钢制造方法

    公开(公告)号:US20100218859A1

    公开(公告)日:2010-09-02

    申请号:US12600161

    申请日:2007-12-27

    摘要: The present invention relates to a high carbon steel sheet that is superior in fatigue life and a method of manufacturing the high carbon steel sheet. The high carbon steel sheet includes about 0.75 wt % to about 0.95 wt % of carbon, smaller than about 1.8 wt % of silicon, about 0.1 wt % to about 1.5 wt % of manganese, about 0.1 wt %˜1.0 wt % of chromium, smaller than about 0.02 wt % of phosphorus, smaller than about 0.02 wt % of sulfur, a residual amount of iron, and inevitable impurities. A layer interval between laminar carbides included in the high carbon steel sheet is smaller than about 0.5 μm. The high carbon steel sheet may include a fine pearlite having a lamellar structure. The fine pearlite included in the high carbon steel sheet may have a volume percentage of larger than about 90%. A ratio of length to width of the lamellar structure may be larger than about 10:1.

    摘要翻译: 本发明涉及疲劳寿命优异的高碳钢板及其制造方法。 高碳钢板包括约0.75重量%至约0.95重量%的碳,小于约1.8重量%的硅,约0.1重量%至约1.5重量%的锰,约0.1重量%至1.0重量%的铬, 小于约0.02重量%的磷,小于约0.02重量%的硫,残留量的铁和不可避免的杂质。 包含在高碳钢板中的层状碳化物之间的层间隔小于约0.5μm。 高碳钢板可以包括具有层状结构的细珠光体。 包含在高碳钢板中的细珠光体可以具有大于约90%的体积百分比。 层状结构的长度与宽度的比可以大于约10:1。

    Manufacturing method of carbon steel sheet superior in formability
    7.
    发明授权
    Manufacturing method of carbon steel sheet superior in formability 有权
    碳钢板的成型性优良的制造方法

    公开(公告)号:US08197616B2

    公开(公告)日:2012-06-12

    申请号:US12158961

    申请日:2006-12-26

    IPC分类号: C21D8/04 C21D8/02

    摘要: A carbon steel sheet having high formability due to a microscopic and uniform carbide distribution and having a good characteristic of final heat treatment, and a manufacturing method thereof. The carbon steel sheet having excellent formability, includes, in wt %, C at 0.2-0.5%, Mn at 0.1-1.2%, Si at less than or equal to 0.4%, Cr at less than or equal to 0.5%, Al at 0.01-0.1%, S at less than or equal to 0.012%, Ti at less than or equal to 0.5×48/14×[N]% when the condition of B(atomic %)/N(atomic %)>1 is satisfied or by 0.5×48/14×[N]% to 0.03% when the condition of B and N is not satisfied, B at 0.0005-0.0080%, N at less than or equal to 0.006%, Fe, and extra inevitable elements; an average size of carbide is less than or equal to 1 μm; and an average grain size of ferrite is less than or equal to 5 μm.

    摘要翻译: 由于碳化物分布微观均匀而具有良好的最终热处理特性的高成形性碳钢板及其制造方法。 具有优异成形性的碳钢板以重量%计含有0.2-0.5%的C,0.1-1.2%的Mn,小于或等于0.4%的Si,小于或等于0.5%的Cr,小于或等于0.5%的Cr 0.01-0.1%,S小于或等于0.012%时,B(原子%)/ N(原子%)> 1的条件为小于或等于0.5×48/14×[N] 满足或当不满足B和N的条件时为0.5×48/14×[N]%至0.03%,B为0.0005-0.0080%,N为小于或等于0.006%,Fe和额外的不可避免的元素 ; 碳化物的平均尺寸小于或等于1μm; 铁素体的平均粒径小于或等于5μm。