摘要:
A toner including: a pigment; polyester resin A that is insoluble in tetrahydrofuran (THF); and polyester resin B that is soluble in THF, wherein the toner satisfies requirements (1) to (3) below: (1) the polyester resin A includes one or more aliphatic diols including from 3 through 10 carbon atoms, as a component constituting the polyester resin A; (2) the polyester resin B includes at least an alkylene glycol in an amount of 40 mol % or more, as a component constituting the polyester resin B; and (3) a glass transition temperature (Tg1st) of the toner at first heating in differential scanning calorimetry (DSC) of the toner is from 20° C. through 50° C.
摘要:
Provided is a resin for a toner, which is a copolymer including a crystalline segment, and having a maximum elastic stress value at 100° C. (ES100) of 1,000 Pa or less, and a maximum elastic stress value at 70° C. (ES70) of 1,000 Pa or greater when the temperature is lowered from 100° C. to 70° C., where the maximum elastic stress values are measured according to a large amplitude oscillatory shear procedure.
摘要:
Provided is a toner containing a binder resin. The binder resin contains a crystalline resin. The toner has a maximum endothermic peak temperature (P1) of from 50° C. to 80° C. and a total endothermic amount (Q) of from 35 J/g to 90 J/g at a first temperature elevation of differential scanning calorimetry. A ratio (Qp/Q) of a total endothermic amount (Qp) of the toner in a temperature range of from 20° C. to the maximum endothermic peak temperature (P1) to the total endothermic amount (Q) of the toner is from 0.65 to 0.83.
摘要:
A toner including: a pigment; polyester resin A that is insoluble in tetrahydrofuran (THF); and polyester resin B that is soluble in THF, wherein the toner satisfies requirements (1) to (3) below:(1) the polyester resin A includes one or more aliphatic diols including from 3 through 10 carbon atoms, as a component constituting the polyester resin A; (2) the polyester resin B includes at least an alkylene glycol in an amount of 40 mol % or more, as a component constituting the polyester resin B; and (3) a glass transition temperature (Tg1st) of the toner at first heating in differential scanning calorimetry (DSC) of the toner is from 20° C. through 50° C.
摘要:
Provided is a resin for a toner, which is a copolymer including a crystalline segment, and having a maximum elastic stress value at 100° C. (ES-100) of 1,000 Pa or less, and a maximum elastic stress value at 70° C. (ES70) of 1,000 Pa or greater when the temperature is lowered from 100° C. to 70° C., where the maximum elastic stress values are measured according to a large amplitude oscillatory shear procedure.
摘要:
A toner includes a binder resin including a copolymer resin (A) having a structural unit derived from a crystalline polyester resin (A1) and another structural unit derived from an amorphous polyester resin (A2), and an amorphous resin (B) in an amount of from 30 to 70% by weight based on total weight of the binder resin. The binarized image of the AFM phase image of the binder resin consists of first phase-contrast images serving as large-phase-difference portions and second phase-contrast images serving as small-phase-difference portions with the first phase-contrast images dispersed in the second phase-contrast images forming a dot-like or streaky structure. The average value of dispersion diameters, corresponding to maximum Feret diameters, of the first phase-contrast images in the dot-like structure, or widths, corresponding to minimum Feret diameters, of the first phase-contrast images in the streaky structure, is less than 100 nm.
摘要:
Toner contains a binder resin containing a crystalline resin having a urethane and/or urea bonding; and a colorant, wherein in a diffraction spectrum of the toner as measured by an X-ray diffraction instrument, a ratio {C/(C+A)} of an integral intensity C of the spectrum derived from the crystalline structure to an integral intensity A of the spectrum derived from the non-crystalline structure is 0.12 or greater, wherein the toner satisfies the following relation 1: T1−T2≦30° C. (Relation 1), where T1 represents the maximum endothermic peak in the first temperature rising from 0° C. to 100° C. at the temperature rising rate of 10° C./min and T2 represents the maximum exothermic peak in the first temperature falling from 100° C. to 0° C. at the temperature falling rate of 10° C./min as T1 and T2 are measured by diffraction scanning calorimetry (DSC).
摘要:
Toner contains a binder resin and a colorant, wherein the binder resin contains a resin having a polyhydroxy carboxylic acid skeleton, wherein the toner has a half effusion temperature of from 80° C. to 120° C. as measured by a temperature rising method using a flow tester.
摘要:
To provide a toner including a binder resin and a colorant, wherein the toner has a glass transition temperature by differential scanning calorimetry (DSC) of 20° C. or greater and less than 50° C., an endothermic peak temperature by DSC of 50° C. or greater and less than 80° C. and an amount of compressive deformation at 50° C. by a thermomechanical analysis of 5% or less.
摘要:
A toner including a colorant and a binder resin is provided. The binder resin includes a polyester resin having a glass transition temperature of 18 to 40° C., a weight average molecular weight of 10,000 to 100,000, and a flow beginning temperature of 70 to 120° C. The toner has a volume average particle diameter of 3 to 10 μm.