Aluminum alloy product and method of making
    2.
    发明授权
    Aluminum alloy product and method of making 失效
    铝合金制品及其制造方法

    公开(公告)号:US3836405A

    公开(公告)日:1974-09-17

    申请号:US27384272

    申请日:1972-07-20

    CPC classification number: C22F1/053 C22C21/10

    Abstract: An aluminum base alloy containing zinc, copper and magnesium together with manganese and with specially controlled composition limits exhibits very high strength when thermally treated to a condition having high resistance to stress corrosion cracking. Improved products of the alloy also exhibit low quench sensitivity and, accordingly, high strength even in very thick sections. A special aging treatment produces the optimum combination of strength and resistance to stress corrosion cracking properties. This invention relates to improved wrought products and to a method of their production.

    Abstract translation: 含有锌,铜和镁以及锰和具有特殊控制组成极限的铝基合金在热处理成具有高抗应力腐蚀开裂性的条件下表现出非常高的强度。 合金的改进产品也具有低的淬火灵敏度,因此即使在非常厚的部分也具有高强度。 特殊的老化处理产生强度和抗应力腐蚀开裂性能的最佳组合。

    Strain hardened aluminum-magnesium alloys
    3.
    发明授权
    Strain hardened aluminum-magnesium alloys 失效
    应变硬化铝镁合金

    公开(公告)号:US3708352A

    公开(公告)日:1973-01-02

    申请号:US3708352D

    申请日:1971-06-14

    CPC classification number: C22C21/06 C22F1/047

    Abstract: ALUMINUM ALLOY PLATE CONTAINING 4.4 TO 10% MAGNESIUM AND STRAIN HARDENED TO IMPROVE ITS STRENGTH TO A LEVEL OF AT LEAST 40% GREATER THAN THE STRENGTH IN THE ANNEALED STATE IS IMPARTED WITH SUBSTANTIALLY FREEDOM FROM SUSCEPTIBILITY OF EXFOLIATION CORROSION. THE PROCESS INCLUDES ROLLING AT MINIMUM TEMPERATURES OF ABOUT 420* TO 650*F. DEPENDING ON THE AMOUNT OF MAGNESIUM PRESENT, TO PRODUCE THE STRAIN HARDENED PRODUCT AND COOLING AT SPECIALLY CONTROLLED RATES.