公开(公告)号:US12054576B2
公开(公告)日:2024-08-06
申请号:US17435758
申请日:2020-03-05
Applicant: BASF SE
Inventor: Berend Eling , Stefan Auffarth , Martin Linnenbrink , Julio Albuerne , Linyu Mu
IPC: C08G18/02 , B32B27/40 , C08G18/09 , C08G18/12 , C08G18/16 , C08G18/22 , C08G18/24 , C08G18/28 , C08G18/42 , C08G18/71 , C08G18/72 , C08G18/76 , C08G18/79 , C08L67/00 , C09J167/02 , C09J175/06 , C09J179/00
CPC classification number: C08G18/025 , B32B27/40 , C08G18/095 , C08G18/12 , C08G18/168 , C08G18/22 , C08G18/227 , C08G18/246 , C08G18/2815 , C08G18/282 , C08G18/2825 , C08G18/4202 , C08G18/4238 , C08G18/71 , C08G18/72 , C08G18/7621 , C08G18/797 , C08L67/00 , C09J167/02 , C09J175/06 , C09J179/00 , C08G2115/06 , C08G2170/20 , C08G2250/00 , C09J2301/304
Abstract: Described herein is a thermosetting resin composition, obtained from the reaction of at least: a polycarbodiimide (i), where the number of carbodiimide groups per molecule is in the range of from 1 to 10; a mixture of crystalline and amorphous polyols (ii), where the molar ratio of carbodiimide groups in the polycarbodiimide according to (i) to hydroxyl groups in the mixture according to (ii) is in the range of from 1:2 to 2:1 and where at least 25 weight-% of the mixture according to (ii) consists of at least one crystalline polyesterol, based on the overall weight of the mixture being 100 weight-%. Also described herein is a method of using the thermosetting resin composition as an adhesive, as well as processes for preparation of adhesives, an element including an adhesive layer on at least one substrate, and an adhesive film, obtained from one of the processes.
-
公开(公告)号:US20220153906A1
公开(公告)日:2022-05-19
申请号:US17435758
申请日:2020-03-05
Applicant: BASF SE
Inventor: Berend Eling , Stefan Auffarth , Martin Linnenbrink , Julio Albuerne , Linyu Mu
IPC: C08G18/02 , C08G18/09 , C08G18/24 , C08G18/16 , C08G18/12 , C08G18/28 , C08G18/42 , C08G18/71 , C08G18/76 , C08G18/79 , C09J175/06
Abstract: Described herein is a thermosetting resin composition, obtained from the reaction of at least: a polycarbodiimide (i), where the number of carbodiimide groups per molecule is in the range of from 1 to 10; a mixture of crystalline and amorphous polyols (ii), where the molar ratio of carbodiimide groups in the polycarbodiimide according to (i) to hydroxyl groups in the mixture according to (ii) is in the range of from 1:2 to 2:1 and where at least 25 weight-% of the mixture according to (ii) consists of at least one crystalline polyesterol, based on the overall weight of the mixture being 100 weight-%. Also described herein is a method of using the thermosetting resin composition as an adhesive, as well as processes for preparation of adhesives, an element including an adhesive layer on at least one substrate, and an adhesive film, obtained from one of the processes.
-