POLYOLEFIN COMPOSITION FOR WATER PIPES WITH INCREASED RESISTANCE TO CHLORINE DIOXIDE
    3.
    发明申请
    POLYOLEFIN COMPOSITION FOR WATER PIPES WITH INCREASED RESISTANCE TO CHLORINE DIOXIDE 审中-公开
    水溶性聚氯乙烯组合物对二氧化氯的耐受性提高

    公开(公告)号:US20130197136A1

    公开(公告)日:2013-08-01

    申请号:US13798809

    申请日:2013-03-13

    Applicant: BOREALIS AG

    Abstract: The present invention relates to a polyolefin composition with increased resistance to degradation caused by ClO2-containing water and to a pipe made of such a polyolefin composition. The present invention further relates to the use of the polyolefin composition for the production of a pipe and to the use of a combination of particular types of antioxidants for increasing the resistance of the polyolefin composition against degradation caused by contact with ClO2-containing water.

    Abstract translation: 本发明涉及由含ClO 2的水引起的对劣化的耐受性提高的聚烯烃组合物和由这种聚烯烃组合物制成的管。 本发明还涉及聚烯烃组合物用于生产管道的用途,以及使用特定类型的抗氧化剂的组合来增加聚烯烃组合物对与含ClO 2的水接触引起的降解的阻力。

    HIGH SPEED CROSS-LINKING OF GRAFTED PLASTOMERS

    公开(公告)号:US20220315716A1

    公开(公告)日:2022-10-06

    申请号:US17276275

    申请日:2019-09-26

    Applicant: BOREALIS AG

    Abstract: The present invention discloses a process for providing a cross-linked composition, the process comprising the steps of (a) providing an ethylene-α-olefin plastomer having—a density of from 850 kg/m3 to 900 kg/m3; and—an melt flow rate (ISO 1133, 2.16 kg, 190° C.) of 0.3 to 50 g/10 min; (b) grafting the ethylene-α-olefin plastomer with silane crosslinker such that the content of silane crosslinker is in the range of 0.1 to 10.0 wt.-% with respect to the grafted ethylene-α-olefin plastomer; (c) contacting said grafted ethylene-α-olefin plastomer with 2 to 8 wt.-% of a tin-free silane crosslinking catalyst with respect to the resulting mixture of grafted ethylene-α-olefin plastomer and tin-freesilane crosslinking catalyst, wherein said tin-free catalyst comprises a Brönsted acid at 23° C. and 50% relative humidity for at least 15 minutes thus forming a cross-linked composition, wherein gel content of said cross-linked composition after 15 min is at least 60%.