Abstract:
Composition comprising a heterophasic propylene copolymer and two different slip agents, namely—a fatty acid amid derivative of formula (I) wherein R1 is a C5 to C25 alkyl residue or C5 to C25 alkenyl residue, R2 is a long-chain organic residue containing at least 6 carbon atoms, and—an unsaturated fatty acid amide.
Abstract:
Heterophasic polypropylene composition comprising (A) 45 to 70 wt % of a propylene homo- or copolymer matrix with an MFR2 in accordance with ISO 1133 (230° C., 2.16 kg load) of ≧80 g/10 min and (B) 25 to 40 wt % of an elastomeric propylene-ethylene copolymer, having an intrinsic viscosity IV (ISO 1628, with decalin as solvent) of ≧3.3 dl/g and an ethylene content of 20 to 50 wt %, (C) 0-15 wt % of an elastomeric ethylene/alpha-olefin random copolymer (D) 3-25 parts per weight of inorganic filler, the heterophasic polypropylene compositions having a total MFR2 (230° C./2.16 kg) in accordance with ISO 1133 of ≧5 g/10 min, a Charpy notched impact strength according to ISO 179/1eA at +23° C. of ≧15.0 kJ/m2, preferably ≧25.0 kJ/m2, a minimum value for the Charpy notched impact strength according to ISO 179/1eA at −20° C. of ≧7.0 kJ/m2, preferably ≧10.0 kJ/m2 and a tensile modulus according to ISO 527-3 of ≧1200 MPa; their preparation and use for producing injection moulded articles being free of flow marks.
Abstract translation:多相聚丙烯组合物,其包含(A)45至70重量%的丙烯均聚物或共聚物基体,其具有根据ISO 1133(230℃,2.16kg负荷)≥80g/ 10min的MFR 2和(B)25 至40重量%的丙烯 - 乙烯共聚物,其特性粘度IV(ISO 1628,作为溶剂的十氢化萘)为≥3.3dl/ g,乙烯含量为20〜50重量%,(C)为0〜15重量% %的弹性体乙烯/α-烯烃无规共聚物(D)3-25重量份的无机填料,根据ISO 1133的总共MFR 2(230℃/ 2.16kg)的多相聚丙烯组合物为≥5g / 10分钟,根据ISO 179 / 1eA在+ 23℃下的夏比缺口冲击强度为≥15.0kJ/ m 2,优选≥25.0kJ/ m 2,根据ISO 179 / 1eA的夏比缺口冲击强度的最小值 在-20℃,≥7.0kJ/ m 2,优选≥10.0kJ/ m 2,并且根据ISO 527-3的≧1200MPa的拉伸模量; 它们的制备和用于生产没有流痕的注塑制品。
Abstract:
Heterophasic polypropylene composition comprising (A) 45 to 70 wt % of a propylene homo- or copolymer matrix with an MFR2 in accordance with ISO 1133 (230° C., 2.16 kg load) of ≧80 g/10 min and (B) 25 to 40 wt % of an elastomeric propylene-ethylene copolymer, having an intrinsic viscosity IV (ISO 1628, with decalin as solvent) of ≧3.3 dl/g and an ethylene content of 20 to 50 wt %, (C) 0-15 wt % of an elastomeric ethylene/alpha-olefin random copolymer (D) 3-25 parts per weight of inorganic filler, the heterophasic polypropylene compositions having a total MFR2 (230° C./2.16 kg) in accordance with ISO 1133 of ≧5 g/10 min, a Charpy notched impact strength according to ISO 179/1eA at +23° C. of ≧15.0 kJ/m2, preferably ≧25.0 kJ/m2, a minimum value for the Charpy notched impact strength according to ISO 179/1eA at −20° C. of ≧7.0 kJ/m2, preferably ≧10.0 kJ/m2 and a tensile modulus according to ISO 527-3 of ≧1200 MPa; their preparation and use for producing injection moulded articles being free of flow marks.