1.
公开(公告)号:US20200148593A1
公开(公告)日:2020-05-14
申请号:US16666876
申请日:2019-10-29
Applicant: Corning Incorporated
Inventor: Hoon Kim , Prantik Mazumder , Aram Rezikyan , Rajesh Vaddi
IPC: C03C27/04 , C03C17/36 , C03C17/245
Abstract: In some embodiments, a method comprises: depositing an adhesion layer comprising manganese oxide (MnOx) onto a surface of a glass or glass ceramic substrate; depositing a first layer of conductive metal onto the adhesion layer; and annealing the adhesion layer in a reducing atmosphere. Optionally, the method further comprises pre-annealing the adhesion layer in an oxidizing atmosphere before annealing the adhesion layer in a reducing atmosphere.
-
公开(公告)号:US20240429375A1
公开(公告)日:2024-12-26
申请号:US18738195
申请日:2024-06-10
Applicant: CORNING INCORPORATED
Inventor: Hoon Kim , Darren Lin , Aram Rezikyan , Cameron Wayne Tanner , Haitao Zhang
Abstract: A battery is provided comprising a coated sintered cathode. The coated sintered cathode comprises at least one of lithium cobalt oxide (LiCoO2) or NMC (LiNi(1-x-y)MnxCoyO2). The coated sintered cathode also comprises a coating layer. The coating layer comprises at least one of aluminum oxide (Al2O3), aluminum fluoride (AlF3), zinc oxide (ZnO), magnesium oxide (MgO), titanium dioxide (TiO2), lanthanum oxide (La2O3), zirconium oxide (ZrO2), gallium oxide (Ga2O3), magnesium fluoride (MgF2), molybdenum trioxide (MoO3), selenium (Se), or phosphorous pentoxide (P2O5). The coating layer is coated on the sintered cathode by atomic layer deposition. The sintered cathode may form a cathode-electrolyte interface inside the battery, and the coating layer may be positioned at the cathode-electrolyte interface.
-
3.
公开(公告)号:US20240140864A1
公开(公告)日:2024-05-02
申请号:US18409103
申请日:2024-01-10
Applicant: CORNING INCORPORATED
Inventor: Hoon Kim , Prantik Mazumder , Aram Rezikyan , Rajesh Vaddi
IPC: C03C27/04 , C03C17/245 , C03C17/36
CPC classification number: C03C27/048 , C03C17/245 , C03C17/3607 , C23C18/1637
Abstract: In some embodiments, a method comprises: depositing an adhesion layer comprising manganese oxide (MnOx) onto a surface of a glass or glass ceramic substrate; depositing a first layer of conductive metal onto the adhesion layer; and annealing the adhesion layer in a reducing atmosphere. Optionally, the method further comprises pre-annealing the adhesion layer in an oxidizing atmosphere before annealing the adhesion layer in a reducing atmosphere.
-
-