公开(公告)号:US20160194476A1
公开(公告)日:2016-07-07
申请号:US14589021
申请日:2015-01-05
Applicant: GENERAL ELECTRIC COMPANY
Inventor: Don Mark LIPKIN , Nicholas Edward ANTOLINO , David POERSCHKE , Kevin Paul MCEVOY
CPC classification number: C08K3/34 , B29C73/02 , B29K2083/00 , C08K3/36 , C08K2003/221 , C08K2003/2213 , C09D183/04 , C08K3/0083 , C08K3/105
Abstract: There is set forth herein a silicon-based patch formulation comprising about 25 to 66 percent by volume of a solvent; about 4 to 10 percent by volume of a silicon-comprising binding material; and about 30 to 65 percent by volume of a patching material, the patching material comprising particles having one or more non-actinide Group IIIA elements, wherein a molar ratio of the one or more non-actinide Group IIIA elements to silicon within the patch formulation is about 0.95 to 1.25.
Abstract translation: 本文提出了含有约25至66%(体积)溶剂的硅基贴片制剂; 约4至10体积%的含硅粘合材料; 和约30至65体积%的修补材料,所述修补材料包含具有一种或多种非锕系IIIA族元素的颗粒,其中所述一种或多种非锕系IIIA族元素与所述贴剂配方中的硅的摩尔比 为约0.95至1.25。
-
公开(公告)号:US20180050964A1
公开(公告)日:2018-02-22
申请号:US15243005
申请日:2016-08-22
Applicant: GENERAL ELECTRIC COMPANY
Inventor: Kevin Paul MCEVOY , James RUUD , Lawrence E. SZALA , Susan CORAH , Atanu SAHA , Hrishikesh KESHAVAN
IPC: C04B35/48 , C23C4/134 , C23C14/22 , C04B35/64 , C04B35/622
CPC classification number: C04B35/48 , C04B35/62222 , C04B35/64 , C04B41/009 , C04B41/5042 , C04B41/87 , C04B2235/5436 , C04B2235/5445 , C04B2235/9607 , C23C4/11 , C23C4/134 , C23C14/221 , C23C28/3455 , F01D5/005 , F01D5/288 , F05B2230/80 , F05B2230/90 , F05C2203/0895 , F05D2300/2118 , Y02T50/6765 , C04B41/4539 , C04B41/4547
Abstract: The present invention is directed to repair compositions for thermal barrier coatings and methods of use thereof. The repair compositions include a ceramic composition, a colloidal solution, an aqueous binder, an aqueous dispersant, and an aqueous ammonia solution. The ceramic composition includes a first population of yttria-stabilized zirconia particles having a mean diameter from about 250 nm to about 1000 nm, a second population of yttria-stabilized zirconia particles having a mean diameter from about 2 μm to about 10 μm, and a third population of yttria-stabilized zirconia particles having a mean diameter from about 20 μm to about 250 μm. One method includes depositing the repair layer onto the damaged region, the repair layer including the repair composition, and heat treating the repair layer.
-