LITHIUM SECONDARY BATTERY AND METHOD OF MANUFACTURING THE SAME
    4.
    发明申请
    LITHIUM SECONDARY BATTERY AND METHOD OF MANUFACTURING THE SAME 有权
    锂二次电池及其制造方法

    公开(公告)号:US20080124631A1

    公开(公告)日:2008-05-29

    申请号:US11771552

    申请日:2007-06-29

    IPC分类号: H01M4/62 H01M10/36 B05D3/00

    摘要: A lithium secondary battery includes an electrode assembly having a positive electrode (1), a negative electrode (2) having a negative electrode current collector and a negative electrode active material layer formed on a surface of the negative electrode current collector and composed of a binder and negative electrode active material particles containing silicon and/or a silicon alloy, and a separator (3) interposed between the electrodes. The electrode assembly is impregnated with a non-aqueous electrolyte. The binder contains a polyimide resin represented by the following chemical formula (1): where R contains at least a benzene ring, and n is within the range of from 10 to 100,000, and the negative electrode active material particles have an average particle size of 5 μm or greater.

    摘要翻译: 锂二次电池包括具有正极(1)的电极组件,负极集电体的负极(2)和形成在负极集电体的表面上并由粘合剂构成的负极活性物质层 和含有硅和/或硅合金的负极活性物质粒子,以及夹在电极之间的隔膜(3)。 电极组件浸渍有非水电解质。 粘合剂含有下述化学式(1)表示的聚酰亚胺树脂:其中,R至少含有苯环,n在10〜100,000的范围内,负极活性物质粒子的平均粒径为 5岁以上。

    Lithium secondary battery and method of manufacturing the same
    5.
    发明授权
    Lithium secondary battery and method of manufacturing the same 有权
    锂二次电池及其制造方法

    公开(公告)号:US08771873B2

    公开(公告)日:2014-07-08

    申请号:US11771552

    申请日:2007-06-29

    IPC分类号: H01M4/13

    摘要: A lithium secondary battery includes an electrode assembly having a positive electrode (1), a negative electrode (2) having a negative electrode current collector and a negative electrode active material layer formed on a surface of the negative electrode current collector and composed of a binder and negative electrode active material particles containing silicon and/or a silicon alloy, and a separator (3) interposed between the electrodes. The electrode assembly is impregnated with a non-aqueous electrolyte. The binder contains a polyimide resin represented by the following chemical formula (1): where R contains at least a benzene ring, and n is within the range of from 10 to 100,000, and the negative electrode active material particles have an average particle size of 5 μm or greater.

    摘要翻译: 锂二次电池包括具有正极(1)的电极组件,负极集电体的负极(2)和形成在负极集电体的表面上并由粘合剂构成的负极活性物质层 和含有硅和/或硅合金的负极活性物质粒子,以及夹在电极之间的隔膜(3)。 电极组件浸渍有非水电解质。 粘合剂含有下述化学式(1)表示的聚酰亚胺树脂:其中,R至少含有苯环,n在10〜100,000的范围内,负极活性物质粒子的平均粒径为 5μm以上。

    Lithium secondary battery and method for manufacturing the same
    6.
    发明授权
    Lithium secondary battery and method for manufacturing the same 有权
    锂二次电池及其制造方法

    公开(公告)号:US08338022B2

    公开(公告)日:2012-12-25

    申请号:US11001192

    申请日:2004-12-02

    IPC分类号: H01M2/02

    摘要: A lithium secondary battery of the present invention comprises a positive electrode formed by disposing a positive-electrode mixture layer containing a positive-electrode active material and a positive-electrode binder, on a surface of a positive-electrode current collector; a negative electrode formed by sintering a negative-electrode mixture layer containing a negative-electrode binder and a negative-electrode active material containing silicon and/or a silicon alloy, disposed on a surface of a negative-electrode current collector; a separator disposed between the positive electrode and the negative electrode; and a nonaqueous electrolyte; wherein an electrode unit obtained by setting the positive electrode and the negative electrode opposed to each other through the separator and rolling them in spirally rolled state is placed in a cylindrical battery container and wherein a curvature radius of the negative-electrode mixture layer opposed to the positive-electrode mixture layer through the separator in the spirally rolled state is 1.5 mm or larger.

    摘要翻译: 本发明的锂二次电池包括在正极集电体的表面上设置含有正极活性物质和正极粘合剂的正极合剂层而形成的正极, 通过在负极集电体的表面上烧结含有负极粘合剂的负极混合层和含有硅和/或硅合金的负极活性物质而形成的负极, 设置在所述正极和所述负极之间的隔膜; 和非水电解质; 其特征在于,将通过隔板相对的正极和负极通过将螺旋卷绕状态进行轧制而得到的电极单元配置在圆筒状的电池容器中,其中与负极混合层相对的曲率半径 螺旋状卷取状态的正极混合层通过隔膜的厚度为1.5mm以上。