    Abstract: The present invention aims to maximize the advantageous physical properties of sulfur and provide a cathode mixture that can be suitably used in a cathode mixture layer of an all-solid-state sodium-sulfur battery in which charge/discharge capacity can be ensured even during operation at normal temperature. The present invention also aims to provide an all-solid-state sodium-sulfur battery including a cathode mixture layer containing the cathode mixture. The present invention relates to a cathode mixture for use in a cathode mixture layer of an all-solid-state sodium-sulfur battery, the cathode mixture including the following components (A) to (C): (A) an ion-conductive material containing phosphorus at a weight ratio of 0.2 to 0.55; (B) sulfur and/or its discharge product; and (C) a conductive material, the component (C) containing a conductive material (C1) having a specific surface area of 1000 m2/g or more.

    Abstract translation: 本发明的目的在于使硫的有利物理性能最大化,并提供可以适用于全固态钠硫电池的阴极混合物层的阴极混合物,其中即使在操作期间也能确保充放电容量 在常温下。 本发明的目的还在于提供一种包含阴极混合物层的全固态钠硫电池。 本发明涉及一种用于全固态钠硫电池的阴极混合层的阴极混合物,该阴极混合物包括以下组分(A)至(C):(A)离子导电材料 含磷重量比为0.2〜0.55; (B)硫和/或其排出产物; 和(C)导电材料,含有比表面积为1000m 2 / g以上的导电材料(C1)的组分(C)。

    POSITIVE-ELECTRODE MIXTURE, MANUFACTURING METHOD THEREFOR, AND ALL-SOLID-STATE LITHIUM-SULFUR BATTERY
    3.
    发明申请
    POSITIVE-ELECTRODE MIXTURE, MANUFACTURING METHOD THEREFOR, AND ALL-SOLID-STATE LITHIUM-SULFUR BATTERY 审中-公开
    阳极电极混合物,其制造方法和全固态锂电池

    公开(公告)号:US20160254529A1

    公开(公告)日:2016-09-01

    申请号:US15027162

    申请日:2014-10-01

    Abstract: The present invention aims to maximize the advantageous physical properties of sulfur and provide a cathode mixture that can be suitably used in a cathode mixture layer of an all-solid-state lithium-sulfur battery having excellent charge/discharge capacity. The present invention also aims to provide an all-solid-state lithium-sulfur battery including a cathode mixture layer containing the cathode mixture. The present invention relates to a cathode mixture for use in a cathode mixture layer of an all-solid-state lithium-sulfur battery, the cathode mixture containing the following components (A) to (D): (A) sulfur and/or its discharge product; (B) elemental phosphorus and/or PxSy where x and y independently represent an integer that gives a stoichiometric ratio; (C) an ion-conductive material; and (D) a conductive material.

    Abstract translation: 本发明的目的在于使硫的有利的物理性质最大化,并提供一种可以适用于具有优异充电/放电容量的全固态锂 - 硫电池的阴极混合物层中的阴极混合物。 本发明的目的还在于提供一种包含阴极混合物层的全固态锂硫电池。 本发明涉及一种用于全固态锂硫电池的阴极混合层的阴极混合物,所述阴极混合物含有以下组分(A)至(D):(A)硫和/或其 放电产品; (B)元素磷和/或PxSy,其中x和y独立地表示给出化学计量比的整数; (C)离子传导材料; 和(D)导电材料。

    POSITIVE ELECTRODE MIXTURE AND ALL-SOLID-STATE LITHIUM SULFUR CELL
    4.
    发明申请
    POSITIVE ELECTRODE MIXTURE AND ALL-SOLID-STATE LITHIUM SULFUR CELL 有权
    正极电极混合物和全固态锂离子电池

    公开(公告)号:US20160118660A1

    公开(公告)日:2016-04-28

    申请号:US14896201

    申请日:2014-03-19

    Abstract: The present invention aims to maximize the advantageous physical properties of sulfur and provide a cathode mixture that can be suitably used in a cathode mixture layer of an all-solid-state lithium sulfur battery exhibiting excellent charge/discharge capacity. The present invention also aims to provide an all-solid-state lithium sulfur battery including a cathode mixture layer containing the cathode mixture. The present invention provides a cathode mixture for use in a cathode mixture layer of an all-solid-state lithium sulfur battery, the cathode mixture containing: (A) an ion-conductive material containing phosphorus at a weight ratio of 0.2 to 0.55; (B) sulfur and/or its discharge product (B); and (C) a conductive material, the amount of the component (B) being 40% by weight or more of the total amount of the components (A), (B), and (C).

    Abstract translation: 本发明的目的在于使硫的有利的物理性能最大化,并提供一种阴极混合物,其可以适用于具有优异充电/放电容量的全固态锂硫电池的阴极混合物层。 本发明还旨在提供一种包括含有阴极混合物的阴极混合物层的全固态锂硫电池。 本发明提供一种用于全固态锂硫电池的阴极混合层的阴极混合物,所述阴极混合物包含:(A)含有重量比为0.2至0.55的磷的离子传导材料; (B)硫和/或其排出产物(B); 和(C)导电材料,组分(B)的量为组分(A),(B)和(C)总量的40重量%以上。