    Abstract: The invention provides novel carbonatable calcium silicate compositions and carbonatable calcium silicate phases that are made from widely available, low cost raw materials by a process suitable for large-scale production. The method of the invention is flexible in equipment and production requirements and is readily adaptable to manufacturing facilities of conventional cement. The invention offers an exceptional capability to permanently and safely sequesters CO2.

    Abstract translation: 本发明提供了通过适用于大规模生产的方法由广泛可得的低成本原料制成的新型碳酸钙硅酸钙组合物和可碳酸钙硅酸钙相。 本发明的方法在设备和生产要求方面是灵活的,并且易于适应常规水泥的制造设施。 本发明提供了永久和安全地螯合二氧化碳的卓越能力。

    LIGHTWEIGHT COMPOSITE MATERIALS PRODUCED FROM CARBONATABLE CALCIUM SILICATE AND METHODS THEREOF
    7.
    发明申请
    LIGHTWEIGHT COMPOSITE MATERIALS PRODUCED FROM CARBONATABLE CALCIUM SILICATE AND METHODS THEREOF 审中-公开
    由碳酸钙生产的轻质复合材料及其制备方法

    公开(公告)号:US20160340261A1

    公开(公告)日:2016-11-24

    申请号:US14715497

    申请日:2015-05-18

    Abstract: An aerated composite material produced from carbonatable calcium silicate compositions (carbonation cured AAC) that has a compressive strength equivalent to autoclaved aerated concrete (ordinary AAC) at substantially the same density and a process of production of the same are provided. The composite material of the present invention comprises: a plurality of bonding elements, each including a core comprising calcium silicate, a first layer which partially or fully surrounds the core and is rich in SiO2, and a second layer which partially or fully surrounds the first layer and is rich in CaCO3; a plurality of filler particles having their particle sizes ranging from 0.1 μm to 1000 μm; and a plurality of voids; wherein the plurality of bonding elements and plurality of filler particles together form a bonding matrix and are substantially evenly dispersed in the matrix and bonded together, the plurality of voids are bubble-shaped and/or interconnected channels, a pore volume with a radius of 0.004 μm to 10.0 μm in the plurality of voids is 0.30 ml/composite material 1 g or less, and a estimated compressive strength expressed by the following formula (1): estimated compressive strength (absolute dry density=0.50)=compressive strength×(0.50÷absolute dry density)2 is 2.0 N/mm2 or greater.

    Abstract translation: 提供了一种由具有与基本相同密度的高压消毒加气混凝土(普通AAC)相当的抗压强度的碳酸钙硅酸盐组合物(碳化固化AAC)生产的充气复合材料及其生产方法。 本发明的复合材料包括:多个结合元件,每个结合元件包括一个包含硅酸钙的芯,第一层,其部分或完全包围该芯并且富含SiO 2;以及第二层,其部分地或完全地围绕第一 层,富含CaCO3; 多个粒径为0.1μm〜1000μm的填料粒子; 和多个空隙; 其中所述多个接合元件和多个填料颗粒一起形成接合基质并且基本均匀地分散在基质中并结合在一起,所述多个空隙是气泡形和/或互连通道,半径为0.004的孔体积 在多个空隙中的微米至10.0μm为0.30ml /复合材料1g或以下,由下式(1)表示的估计抗压强度:估计的抗压强度(绝对干密度= 0.50)=抗压强度×(0.50 ÷绝对干密度)2为2.0N / mm2以上。